Patents
US 8,308,858 B2#10856232 Most CitedActiveUnited States (USPTO)Utility

Electroless deposition process on a silicon contact

10Forward Citations (#10856232 Global)
0.7/yrCitation Velocity (#10740540 Global)
1.50Citation PageRank (#22927707 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Embodiments as described herein provide methods for depositing a material on a substrate during electroless deposition processes, as well as compositions of the electroless deposition solutions. In one embodiment, the substrate contains a contact aperture having an exposed silicon contact surface. In another embodiment, the substrate contains a contact aperture having an exposed silicide contact surface. The apertures are filled with a metal contact material by exposing the substrate to an electroless deposition process. The metal contact material may contain a cobalt material, a nickel material, or alloys thereof. Prior to filling the apertures, the substrate may be exposed to a variety of pretreatment processes, such as preclean processes and activations processes. A preclean process may remove organic residues, native oxides, and other contaminants during a wet clean process or a plasma etch process. Embodiments of the process also provide the deposition of additional layers, such as a capping layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 10.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A composition of an activation solution, comprising: a cobalt source at a concentration within a range from about 1 mM to about 100 mM; a fluoride source at a concentration within a range from about 10 mM to about 400 mM; and a hypophosphite source at a concentration within a range from about 5 mM to about 150 mM.

  2. Claim 2Depends on #1

    The composition of claim 1 , further comprising: a cobalt source at a concentration within a range from about 5 mM to about 50 mM; a fluoride source at a concentration within a range from about 20 mM to about 200 mM; and a hypophosphite source at a concentration within a range from about 10 mM to about 80 mM.

  3. Claim 3Depends on #2

    The composition of claim 2 , further comprising: the cobalt source at a concentration within a range from about 10 mM to about 30 mM; the fluoride source at a concentration within a range from about 50 mM

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 2,369,620 AMethod of coating cupreous metal with tin1945288
US 3,403,035 AProcess for stabilizing autocatalytic metal plating solutions196867
US 3,745,039 AElectroless cobalt plating bath and process197357
US 3,937,857 ACatalyst for electroless deposition of metals1976324
US 4,006,047 ACatalysts for electroless deposition of metals on comparatively low-temperature polyolefin and polyester substrates1977316
US 4,072,781 AMagnetic recording medium197839
US 4,150,177 AMethod for selectively nickeling a layer of polymerized polyester resin197940
US 4,232,060 AMethod of preparing substrate surface for electroless plating and products produced thereby1980277
US 4,234,628 ATwo-step preplate system for polymeric surfaces1980276
US 4,239,810 AMethod of making silicon photovoltaic cells198055
US 4,265,943 AMethod and composition for continuous electroless copper deposition using a hypophosphite reducing agent in the presence of cobalt or nickel ions1981337
US 4,297,393 AMethod of applying thin metal deposits to a substrate198132
US 4,364,803 ADeposition of catalytic electrodes on ion-exchange membranes1982276
US 4,366,035 AElectrodeposition of gold alloys198216
US 4,368,223 AProcess for preparing nickel layer1983292
US 4,397,812 AElectroless nickel polyalloys1983316
US 4,424,241 AElectroless palladium process198479
JP S59215473 ASolution for holding activity of copper film formed by electroless plating—5
US 4,632,857 AElectrolessly plated product having a polymetallic catalytic film underlayer1986275
US 4,717,591 APrevention of mechanical and electronic failures in heat-treated structures198835