PAEK powder, in particular for the use in a method for a layer-wise manufacturing of a three-dimensional object, as well as method for producing it
Abstract
By a temper treatment a polyaryletherketone powder is processed such that it is particularly suited for the use in a method for a layer-wise manufacturing of a three-dimensional object. To this effect the powder is tempered at a temperature that is at least 20° C. above the glass transition temperature for at least 30 minutes before it is used as building material.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 9.
Claims (3 — 3 Independent, 0 Dependent)
- Claim 1Independent Claim
Polyaryletherketone(PAEK) fine powder for the use as building material in a method for a layer-wise generation of three-dimensional objects, wherein the PAEK fine powder has a melt viscosity that lies below 0.25 kN*s/m 2 , a D 0.90 -value below 150 μm, a BET surface below 40 m 2 /g and a bulk density having a value equal to or larger than 0.42 g/cm 2 .
- Claim 2Independent Claim
Polyaryletherketone(PAEK) fine powder for the use as building material in a method for a layer-wise generation of three-dimensional objects, wherein the PAEK fine powder has a melt viscosity between 0.25 kN*s/m 2 and 0.50 kN*s/m 2 , a D 0.90 -value below 150 μm, a BET surface below 40 m 2 /g and a bulk density having a value which is equal to or larger than 0.39 g/cm 2 .
- Claim 3Independent Claim
Polyaryletherketone(PAEK) fine powder for the use as building material in a method for a layer-wise generation of three-d
Technical Overview & Description