US 8,288,476 B2#44598106 Most CitedActiveUnited States (USPTO)Utility

Golf ball material, golf ball and method for preparing golf ball material

2Forward Citations (#44598106 Global)
0.1/yrCitation Velocity (#39967977 Global)
0.90Citation PageRank (#47697827 Global)
17Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention provides a golf ball material composed of (i) a non-ionomeric thermoplastic resin, (ii) an ionomeric resin and/or an acid-containing polymer which is the base polymer of an ionomeric resin, and (iii) a norbornene dicarboxylic anhydride and/or a derivative thereof. Methods for preparing such a material, and a golf ball which includes as a component therein a part made of the golf ball material are also provided. The golf ball material has a good thermal stability, flow and processability, and can thus be used to obtain high-performance golf balls endowed with an excellent rebound resilience, durability and flexibility.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 2.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a golf ball material, comprising the steps of, in order, melt-blending (iii) a norbornene dicarboxylic anhydride and/or a derivative thereof, a peroxide, and (i) a non-ionomeric thermoplastic resin that is not a polyester elastomer in a temperature range at which the peroxide does not decompose too soon; adding (ii) an acid-containing polymer that is the base polymer of an ionomeric resin; and melt-mixing at the temperature or above at which the peroxide decomposes.

  2. Claim 2Depends on #1

    The method for preparing a golf ball material of claim 1 , wherein the peroxide is selected from among compounds having a 1-minute half-life decomposition temperature in a range of 140 to 250° C., and is added in an amount of 0.05 to 15 parts by weight per 100 parts by weight of the combined amount of the resin ingredients.

  3. Claim 3Independent Claim

    The method for preparing a gol

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Computer translation of JP2003183484; no date.