hottub.patents
US 8,288,274 B2#38109376 Most CitedActiveUnited States (USPTO)Utility

Method of forming noble metal layer using ozone reaction gas

2Forward Citations (#38109376 Global)
0.1/yrCitation Velocity (#39688537 Global)
1.07Citation PageRank (#37879938 Global)
11Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A noble metal layer is formed using ozone (O 3 ) as a reaction gas.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming a noble metal layer, comprising: performing a deposition process by using a noble metal source and a reaction gas, the reaction gas consisting essentially of ozone (O 3 ), wherein the ozone has a first concentration level ranging from approximately 20 g/m 3 to approximately 100 g/m 3 , and wherein the noble metal layer is formed over a substrate at a substrate temperature ranging from approximately 150° C. to approximately 275° C.; and performing an etch process using ozone having a concentration level of ranges from approximately 200 g/m 3 to approximately 350 g/m 3 .

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the performing of the deposition process comprises using an atomic layer deposition (ALD) method, the ALD method comprising repeatedly performing supplying the noble metal source, purging, supplying the ozone as the reaction gas, and purg

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Chinese Office Action for Chinese application No. 200910001299.1, citing the attached reference(s), Apr. 22, 2010.
  • Nakahara, M., et al., "Etching technique for ruthenium with a high etch rate and high selectivity using ozone gas", J. Vac. Sci. Technol. B 19(6), Nov./Dec. 2001, pp. 2133-2136.