Patents
US 8,257,488 B2#60074970 Most CitedActiveUnited States (USPTO)Utility

Cementitious compositions having coarse ground blast furnace slag and methods of making and using the same

1Forward Citations (#60074970 Global)
0.1/yrCitation Velocity (#51208388 Global)
0.77Citation PageRank (#60074970 Global)
38Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A cementitious composition capable of forming a high, early-phase strength cement may comprise construction grade cement and ground blast furnace slag, the ground blast furnace slag having a Blaine fineness less than about 250 m 2 /kg. The cementitious composition may comprise, for each 100% by weight, greater than about 50% by weight construction grade portland cement and less than about 50% by weight ground blast furnace slag, and the cementitious composition may have a Blaine fineness less than about 300 m 2 /kg. Methods of making and using such a cementitious composition to cement a structure are also described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 38 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A cementitious composition comprising: construction grade cement at about 70% by weight; ground blast furnace slag at about 30% by weight; wherein the ground blast furnace slag has a Blaine fineness of about 139 m 2 /kg; wherein the construction grade cement has a Blaine fineness of about 290 m 2 /kg; and wherein the cementitious composition has a Blaine fineness of about 242 m 2 /kg.

  2. Claim 2Depends on #1

    The cementitious composition of claim 1 wherein the ground blast furnace slag comprises by weight about 35% SiO 2 , about 16% Al 2 O 3 , about 38% CaO, about 6% MgO, about 0.95% Fe 2 O 3 , about 1.2% MnO 2 , about 0.4% K 2 O, about 0.3% Na 2 O, and about 1.05% S.

  3. Claim 3Depends on #1

    The cementitious composition of claim 1 wherein the cementitious composition comprises by weight about 25.48% SiO 2 , about 8.45% Al 2 O 3 , about 1.57% Fe 2 O 3 , about 57.38% CaO, ab

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (38)

PatentTitleYearCitations
US 4,223,733 AMethod for cementing oil wells198015
US 4,761,183 AGrouting composition comprising slag1988130
US 5,026,215 AMethod of grouting formations and composition useful therefor199153
JP H03170354 AUltrahigh early strength cement composition—7
US 5,049,288 ASet retarded cement compositions and methods for well cementing1991136
US 5,071,484 ACementitious compositions and method199141
US 5,086,850 AWell bore drilling direction changing method1992127
US 5,121,795 ASqueeze cementing1992221
US 5,123,487 ARepairing leaks in casings1992188
US 5,125,455 APrimary cementing1992224
US 5,127,473 ARepair of microannuli and cement sheath1992209
US 5,181,568 AMethods of selectively reducing the water permeabilities of subterranean formations199386
US 5,238,064 ASqueeze cementing1993101
US 5,284,513 ACement slurry and cement compositions199449
US 5,311,944 ABlast furnace slag blend in cement199419
US 5,340,397 ASet retarded ultra fine cement compositions and methods199479
JP H0769704 ARapidly curable self-leveling plaster—12
US 5,547,024 AMethod of using construction grade cement in oil and gas wells199623
US 5,578,122 AMethods of producing concretes containing class C fly ash that are stable in sulphate environments199615
US 5,658,624 AArticles formed by extruding hydraulically settable compositions199775
US 5,976,243 AProcess for producing cement clinker containing blast furnace slag199929
US 6,113,684 ARapid hardening, ultra-high early strength Portland-type cement compositions, novel clinkers and methods for their manufacture which reduce harmful gaseous emissions200062
US 6,273,191 B1Cementing casing strings in deep water offshore wells200146
US 6,336,505 B1Cementing casing strings in deep water offshore wells200238
US 6,406,534 B1Rapid hardening, ultra-high early strength portland-type cement compositions, novel clinkers and methods for their manufacture which reduce harmful gaseous emissions200225
US 6,454,004 B2Cementing casing strings in deep water offshore wells200249
US 6,630,021 B2Cementing casing strings in deep water offshore wells200342
GB 2,387,593 AImpermeable oil well cement—20
US 6,758,896 B2Rapid hardening, ultra-high early strength portland-type cement compositions, novel clinkers and methods for their manufacture which reduce harmful gaseous emissions200416

Non-Patent Literature (5)

  • Bentz et al. "Early-Age Properties of Cement-Based Materials I: Influence of Cement Fineness" Journal of Materials in Civil Engineering, 502, (Jul. 2008), 502-508 (7 pages).
  • Labarca et al. "Effects of Ground Granulated Blast Furnace Slag in Portland Cement Concrete-Expanded Study" (available at http://on.dot.wi.gov/wisdotresearch/database/reports/05-01slagexpanded-fr.pdf) (Jun. 2007), (89 pages).
  • Office Action dated Mar. 16, 2011 in parent U.S. Appl. No. 12/357,256, issued as U.S. Patent No. 8,056,631.
  • Office Action dated Mar. 4, 2010 in parent U.S. Appl. No. 12/357,256, issued as U.S. Patent No. 8,056,631.
  • Office Action dated Sep. 1, 2010 in parent U.S. Appl. No. 12/357,256, issued as U.S. Patent No. 8,056,631.