RTP spike annealing for semiconductor substrate dopant activation
Abstract
A semiconductor substrate has a plurality of active device patterns. At least some of the active device patterns comprise doped regions. The substrate has a plurality of surface regions, including the active device patterns and un-patterned regions, with respectively different reflectances for light in a near infrared wavelength. A first difference is determined, between a largest reflectance at the near infrared wavelength and a smallest reflectance at the near infrared wavelength. A second infrared wavelength is determined, for which a second difference between a largest reflectances a smallest reflectance is substantially less than the first difference at the near infrared wavelength. A rapid thermal processing (RTP) spike annealing dopant activation step is performed on the substrate using a second light source providing light at the second wavelength.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 5.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method comprising: providing a semiconductor substrate having a plurality of patterns formed thereon or therein, at least some of the patterns comprising doped regions, the substrate having a plurality of surface regions, including the patterns and un-patterned regions, with respectively different reflectances for light in a near infrared wavelength; and performing a rapid thermal processing (RTP) spike annealing dopant activation step on the substrate using far infrared light, wherein a difference between a largest one of the different reflectances and a smallest one of the different reflec
- Claim 2Depends on #1
The method of claim 1 , wherein a difference between a largest one of the different reflectances and a smallest one of the different reflectances at the near infrared wavelength is about 0.47.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (23)
Non-Patent Literature (4)
- Corresponding Chinese Application No. 200910162398.8 Office Action Jul. 13, 2011, pp. 1-3.
- Erik Bründermann et al., First operation of a far-infrared p-germanium laser in a standard close-cycle machine at 15 K' Jun. 1997, Infrared Physics & Technology, vol. 38, Issue 4, pp. 201-203.
- J. Harnish and C. Carlson of Micron Technology, Inc., and J. Foggiato, K. Kang and W.S.Yoo of WaferMasters, Inc. Electrical Activation and Dopant Diffusion of Heavily Boron Implanted Silicon. This paper appears at: www.wafermasters.com/Publications/ECS2005-K1-1513O%20 Harnish.pdf. USA.
- Woo Sik Yoo and Kitaek Kang of WaferMasters Inc., San Jose, CA. Rapid Thermal Scanning for Dopant Activation for Advanced Junction Technology. This paper appears in: Junction Technology, 2007 International Workshop, Publication Date: Jun. 8-9, 2007, on pp. 119-120. ISBN: 1-4244-1103-3. USA.