Abstract

An interconnector is made of ferritic chromium steel, on which a cupriferous layer is disposed. This layer prevents interdiffusion between the chromium steel and additional components with which the interconnector has direct contact. According to the state of the art, such diffusion occurs particularly if these additional components contain nickel. In addition, the interconnector may comprise a chromium-containing oxide layer as a barrier against interdiffusion. For this purpose, the interconnector steel can also be preoxidized before applying the cupriferous layer. The interconnector has a significantly longer service life than interconnectors according to the state of the art, and it has improved electrical conductivity because the electrical contact surface thereof is free of oxides and has high transverse conductivity.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An interconnector for a fuel cell made of ferritic chromium steel, comprising a cupriferous layer including at least 50 wt % copper or copper alloy, disposed in at least some regions of the surface thereof, and an additional chromium-containing oxide layer made of Cr 2 O 3 disposed at the interface between the cupriferous layer and the chromium steel, and wherein the cupriferous layer does not oxidize in an operating atmosphere of a fuel cell that includes the interconnector, the operating atmosphere including an oxidizing agent.

  2. Claim 2Depends on #1

    The interconnector according to claim 1 , comprising a further oxide layer is disposed within the cupriferous layer.

  3. Claim 3Depends on #1, #2

    An interconnector according to any one of claim 1 or 2 , wherein the Cr 2 O 3 layer has a thickness of between 0.2 and 3 mm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
DE 19,913,873 A1High temperature fuel cell has an interconnector coated with a nickel layer and an overlying layer to prevent oxidation—4
WO 0,059,057 A1High-temperature fuel cell—4
CN 2,400,908 YAnode film-connection board struture for use in solid oxide fuel cell stack20005
US 6,326,096 B1Solid oxide fuel cell interconnector200158
US 2002094465 A1High-temperature fuel cell—19
WO 02,058,169 A2The use of sulfur-containing fuels for direct oxidation fuel cells—12
US 6,492,053 B1Planar fuel cell assembly2002148
US 2003224234 A1Forming an impermeable sintered ceramic electrolyte layer on a metallic foil substrate for solid oxide fuel cell—24
DE 10,306,647 A1Herstellungsverfahren für eine Schutzschicht für hochtemperaturbelastete, chromoxidbildende Substrate—16
DE 10,306,649 A1Schutzschicht für hochtemperaturbelastete Substrate, sowie Verfahren zur Herstellung derselben—33
CN 1,667,859 AProcess for preparing solid oxide fuel battery connectors—9
US 2006286433 A1Interconnects for solid oxide fuel cells and ferritic stainless steels adapted for use with solid oxide fuel cells—27
WO 2006/138070 A1Interconnects for solid oxide fuel cells and ferritic stainless steels adapted for use with solid oxide fuel cells—18
US 7,390,582 B2Method for producing a protective coating for substrates that are subjected to high temperatures and form chromium oxide200811
US 7,407,717 B2Protective coating for substrates that are subjected to high temperatures and method for producing said coating200810

Non-Patent Literature (1)

  • Michalik M et al: "Effect of component thickness on lifetime and oxidation rate of chromia forming ferritic steels in low and high p02 environments" Materials At High Temperatures, Butterworth Heinemann, Guildford, GB, vol. 22, No. 3-4, 2005, pp. 213-221, XP008083919 ISSN: 0960-3409 p. 214, left-han