Patents
US 8,218,271 B2#100094500 Most CitedActiveUnited States (USPTO)Utility

TMR sensor with a multilayered reference layer

0Forward Citations (#100094500 Global)
0.0/yrCitation Velocity (#100094500 Global)
0.56Citation PageRank (#100094500 Global)
38Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

According to one embodiment, a method for forming at least a portion of a magnetic head includes forming a keeper layer, forming a reference layer, and forming an AFM coupling layer which is positioned between the keeper layer and the reference layer. In addition, forming the reference layer includes forming a layer of CoFe, depositing a layer of CoFeHf which is about 20 atomic % Hf, and depositing a layer of CoFeB such that the layers of CoFeHf and CoFeB are directly adjacent and a ratio of respective physical thicknesses of CoFeHf to CoFeB is less than about 0.66. Other embodiments are also included such as a magnetic head and additional methods for forming at least a portion of a magnetic head.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 38 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for forming at least a portion of a magnetic head, the method comprising: forming a keeper layer; forming a reference layer; forming an AFM coupling layer, the AFM coupling layer being positioned between the keeper layer and the reference layer; and wherein forming the reference layer includes: forming a layer of CoFe; depositing a layer of CoFeHf, wherein the layer of CoFeHf is about 20 atomic % Hf; depositing a layer of CoFeB, wherein the layers of CoFeHf and CoFeB are directly adjacent; and depositing a second layer of CoFe above the layers of CoFeHf and CoFeB.

  2. Claim 2Depends on #1

    The method as recited in claim 1 , wherein depositing the layer of CoFeHf is performed by co-sputtering CoFe and Hf, wherein a Hf and a CoFe deposition power are each selected and used to provide a HeP 2 of the reference and keeper layers of greater than about 3500 Oe.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (38)

PatentTitleYearCitations
US 6,262,869 B1Spin valve sensor with encapsulated keeper layer and method of making200197
US 6,327,122 B1Spin valve sensor having antiparallel (AP) pinned layer with high resistance and low coercivity200117
US 6,519,121 B1Spin valve sensor with composite pinned layer structure for improving biasing of free layer structure with reduced sense current shunting200327
US 6,525,911 B1Permeability offset of shield layers for correcting bias of a free layer structure in a spin valve sensor200318
US 6,600,638 B2Corrosion resistive GMR and MTJ sensors200343
US 2004041183 A1Amorphous alloys for magnetic devices—53
US 6,713,195 B2Magnetic devices using nanocomposite materials200448
US 6,723,457 B2Perpendicular magnetic recording media, manufacturing process of the same, and magnetic storage apparatus using the same200426
US 6,731,477 B2Current-perpendicular-to-plane spin-valve sensor with metallic oxide barrier layer and method of fabrication200435
US 6,818,458 B1Methods involving a low resistance magnetic tunnel junction structure200424
US 6,891,703 B2Exchange coupled film having magnetic layer with non-uniform composition and magnetic sensing element including the same20057
US 7,001,680 B2Low resistance magnetic tunnel junction structure200612
US 7,041,205 B2Sputtering target and method for making composite soft magnetic films with a sintered target20063
US 7,067,331 B2Method of making amorphous alloys for semiconductor device200641
US 7,102,854 B2Transducing head with reduced side writing200642
US 7,149,045 B1Longitudinal media with soft underlayer and perpendicular write head200647
US 7,227,728 B2Method and apparatus for a current-perpendicular-to-plane Giant Magneto-Resistance sensor with embedded composite film200714
US 7,242,556 B2CPP differential GMR sensor having antiparallel stabilized free layers for perpendicular recording200739
US 2007217088 A1Method and apparatus for providing magnetostriction control in a freelayer of a magnetic memory device—15
US 2007230068 A1Dual-type tunneling magnetoresistance (TMR) elements—18
US 2008023740 A1Novel capping layer for a magnetic tunnel junction device to enhance dR/R and a method of making the same—55
US 7,345,854 B2GMR sensor having a reference layer with movable magnetization200825
US 2008080101 A1Dual-layer free layer in a tunneling magnetoresistance (tmr) element—39
US 2008144234 A1Current-perpendicular-to-plane sensor with dual keeper layers—22
US 2008204945 A1Magnetoresistance sensors pinned by an etch induced magnetic anisotropy—11
US 2008259507 A1Tunneling Magnetoresistive (TMR) Sensor with A Co-Fe-B Free Layer Having A Negative Saturation Magnetostriction—20
US 7,461,933 B2Sheet heater assembly having air bearing platelets200816
US 7,486,475 B2Magnetic data system having bias circuit with bias resistor200919
US 2009168267 A1Current-perpendicular-to-plane (cpp) read sensor with multiple reference layers—19
US 7,633,724 B2Dual-type tunneling magnetoresistance (TMR) elements20093