Cushion for polishing pad and polishing pad using the cushion
Abstract
The invention provides a cushion for a polishing pad, wherein, when a dynamic compression viscoelasticity measurement is performed under conditions of 23° C., a static load of 27.6 kPa, a frequency of 11 Hz and an amplitude of 1 μm, (1) a phase difference between dynamic stress and deformation is 4° or less, and (2) a ratio of the maximum value of the deformation amount to the maximum value of the dynamic stress ([maximum value of deformation amount]/[maximum value of dynamic stress]) is 0.5 μm/kPa or more. The invention also provides a polishing pad having a layer of the cushion for a polishing pad and a polishing layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A polishing pad having a cushion layer and a polishing layer, wherein the cushion layer comprises polyurethane, chloroprene rubber, or silicone rubber, the polishing layer comprises a polymer material having a tensile elastic modulus at 50° C. after saturation swelling with water at 50° C. of 130 to 800 MPa, a loss tangent at 50° C. of 0.2 or less, and a contact angle with water of 80° or less, and when a dynamic compression viscoelasticity measurement is performed on the cushion layer under conditions of 23° C., a static load of 27.6 kPa, a frequency of 11 Hz and an amplitude of 1 μm, (1) a p
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.