Patents
US 8,206,645 B2#117823805 Most CitedActiveUnited States (USPTO)Utility

Preparation of filler-metal weld rod by injection molding of powder

0Forward Citations (#117823805 Global)
0.0/yrCitation Velocity (#117823805 Global)
0.56Citation PageRank (#117823805 Global)
39Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for preparing a filler-metal weld rod of a filler-metal composition includes the steps of centerless grinding the filler metal weld rod of a forced mixture of a mass of titanium aluminide intermetallic alloy powder that was used to form the weld rod, and hot isostatic pressing the filler-metal weld rod at a temperature greater than 2150° F., at a pressure between about 15,000 pounds per square inch and about 25,000 pounds per square inch and for a time of about 1 to 5 hours, thereby increasing the relative density to between about 98% and about 99%.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 39 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a filler-metal weld rod of a filler-metal composition, comprising the steps of: centerless grinding the filler metal weld rod of a forced mixture of a mass of titanium aluminide intermetallic alloy powder that was used to form the weld rod; and thereafter hot isostatic pressing the filler-metal weld rod at a temperature greater than 2150° F., at a pressure between about 15,000 pounds per square inch and about 25,000 pounds per square inch and for a time of about 1 to 5 hours, thereby increasing the relative density to between about 98% and about 99%.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the titanium aluminide intermetallic alloy powder has a nominal filler-metal composition in atomic percent of from about 45.5 to about 48.0 percent aluminum and from about 48 to about 50.5 percent titanium, with the balance other elements.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (39)

PatentTitleYearCitations
US 3,701,444 AFlexible welding rod having organically bound core and protective sheath197221
US 4,129,462 AGamma prime hardened nickel-iron based superalloy197824
US 4,213,026 AAge hardenable nickel superalloy welding wires containing manganese198029
US 4,426,428 ANickel-base welding electrode198439
JP S6117398 AProduction of high alloy welding rod—5
US 4,624,706 AWeld wire from extruded nickel containing powder198618
EP 0,208,496 A1Weld wire from extruded nickel containing powder—5
US 4,673,123 AFiller for welding a heat resistant nickel-base alloy198715
US 4,846,885 AHigh molybdenum nickel-base alloy198912
US 5,051,112 AHard facing199153
JP H03232904 AExtruded green compact of alloy powder and sintered product thereof—7
JP H055105 AMethod for extruding alloy powder and production of sintered product of alloy powder—3
JP H05115995 ABuild-up material for member made of tial, ti3al intermetallic compound and valve made of tial, ti3al intermetallic compound—4
US 5,332,628 AIron based ductile wire for forming a surfacing alloy system199439
US 5,453,243 AMethod for producing titanium aluminide weld rod199511
US 5,525,779 AIntermetallic alloy welding wires and method for fabricating the same199640
US 5,682,665 AMethod for manufacturing a dental curette199752
US 5,989,493 ANet shape hastelloy X made by metal injection molding using an aqueous binder199940
DE 19,935,276 A1Production of components used e.g. in vehicle construction comprises injection molding metal powder particles coated with a binder in a mold, removing the binder and sintering—28
WO 0,012,248 A1Powder metal injection molding process for forming an article from the nickel-based superalloy 'hastelloy x'—4
JP 2000328103 ADebinder method of ti-al based alloy injection molding body and dewaxing device of powder molding body for the same—16
US 6,238,498 B1Method of fabricating a homogeneous wire of inter-metallic alloy200111
US 6,300,588 B1Manufacture of repair material and articles repaired with the material200113
US 6,361,739 B1Fabrication process for high density powder composite hardfacing rod200213
US 6,440,358 B1Fabrication process for powder composite rod200213
US 6,465,755 B2Manufacture of repair material and articles repaired with the material20028
US 6,482,352 B1Method of manufacturing watch-bracelet component200213
US 2002178862 A1Tungsten-carbide articles made by metal injection molding and method—28
EP 1,287,943 A1Method of manufacturing a nickel-base alloy welding filler metal—4
US 2003042233 A1Production and use of welding filler metal—14

Non-Patent Literature (1)

  • Valencia J.J. et al.: "Microstructure and mechanical properties of inconel 625 and 718 alloys processed by powder injection molding." Proceedings of the International Symposium on Superalloys 718, 625, 706 and Various Derivatives, 1994, pp. 935-945, XP008059325 Warrendale, PA 15086.