Patents
US 8,202,808 B2#33361206 Most CitedActiveUnited States (USPTO)Utility

Methods of forming strontium titanate films

3Forward Citations (#33361206 Global)
0.2/yrCitation Velocity (#32472994 Global)
1.04Citation PageRank (#39389128 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the current invention include methods of forming a strontium titanate (SrTiO 3 ) film using atomic layer deposition (ALD). More particularly, the method includes forming a plurality of titanium oxide (TiO 2 ) unit films using ALD and forming a plurality of strontium oxide (SrO) unit films using ALD. The combined thickness of the TiO 2 and SrO unit films is less than approximately 5 angstroms. The TiO 2 and SrO units films are then annealed to form a strontium titanate layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming a strontium titanate film, comprising: a. applying between 50 and 200 pre-saturation pulses without a pulse of an oxidant between the pulses of a Sr-precursor to a substrate, wherein the substrate comprises a conductive layer; b. forming a Sr-containing and Ti-containing film on the substrate after applying the pulses by i. forming an SrO film from one or more SrO unit films; ii. forming a TiO 2 film from one or more TiO 2 unit films over the previously formed SrO film; iii. forming one or more SrO unit films over the previously formed TiO 2 film if the combined total t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗