Patents
US 8,197,939 B2#37394250 Most CitedActiveUnited States (USPTO)Utility

Method for producing a flexible composite elastomeric polyurethane skin

2Forward Citations (#37394250 Global)
0.1/yrCitation Velocity (#39642356 Global)
1.11Citation PageRank (#36216928 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a method for producing a flexible elastomeric composite polyurethane skin comprising a first and a second flexible polyurethane layer obtained by spraying a first and a second polyurethane reaction mixture onto one another. The first reaction mixture is an aliphatic polyurethane reaction mixture which is free of lead and formulated to produce a polyurethane elastomer having a flexural modulus smaller than 35 MPa. The second reaction mixture is an aromatic polyurethane reaction mixture producing a polyurethane elastomer having a smaller flexural modulus. The thickness of the aliphatic polyurethane layer could be made so small with respect to the thickness of the aromatic polyurethane layer that the composite skin has an average flexural modulus smaller than 30 MPa. Notwithstanding the lower reactivity of the aliphatic polyurethane reaction mixture, especially when using a higher NCO-index to reduce the “rubbery feel” and the emission of VOCs and/or a flexibiliser to achieve a higher flexibility, sufficiently short cycle times can be achieved due to the accelerated curing observed when spraying the aromatic polyurethane sufficiently early against the

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a flexible elastomeric composite polyurethane skin having an average areal weight of at least 0.6 kg/m 2 and an average flexural modulus, measured in accordance with ASTM D790-03, smaller than 30 MPa, preferably smaller than 25 MPa and more preferably smaller than 20 MPa, which method comprises the steps of: providing a first polyurethane reaction mixture; spraying a layer of said first polyurethane reaction mixture onto a mould surface to produce a first elastomeric polyurethane layer having a first flexural modulus; providing a second polyurethane reaction mixture whi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)