Patents
US 8,192,562 B2#20965130 Most CitedActiveUnited States (USPTO)Utility

Spring steel wire excellent in fatigue characteristic and wire drawability

5Forward Citations (#20965130 Global)
0.4/yrCitation Velocity (#21996154 Global)
1.47Citation PageRank (#23601176 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An object of the preset invention is to provide a spring steel wire that: shows excellent wire drawability not only when it is used as a spring steel wire for cold-winding formed into a steel spring by applying quenching and tempering treatment after wiredrawing but also when it is used as a spring steel wire for cold-winding formed into a steel spring as it is wiredrawn; and secures a spring having an excellent fatigue characteristic after the spring steel wire is formed into the spring. The spring steel wire according to the present invention is a spring steel wire excellent in fatigue characteristic and wire drawability, wherein: the contents of C, Si, Mn, Cr, Ti, B, and other elements are specified; the contents (mass %) of B, Ti, and N satisfy the expression (1) below; the amount of solid solute B is in the range of 0.0005% to 0.0040%; the remainder in the spring steel wire is composed of Fe and unavoidable impurities; and the solid solute B concentrates at the grain boundaries of pearlite nodules, 0.03≦B/(Ti/3.43−N)≦5.0 (1).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A spring steel wire excellent in fatigue characteristic and wire drawability wherein: said spring steel wire contains C: 0.50%-0.70%, Si: 1.0%-2.5%, Mn: 0.5%-1.5%, Cr: 0.5%-1.5%, Ti: 0.005%-0.10%, B: 0.0010%-0.0050%, N: 0.005% or less, P: 0.015% or less, S: 0.015% or less, Al: 0.03% or less, and O: 0.0015% or less; wherein for each chemical component, % means mass %; the contents (mass %) of B, Ti, and N satisfy the expression (1): 0.03≦B/(Ti/3.43−N)≦5.0  (1); the amount of solid solute B is in the range of 0.0005% to 0.0040%; the remainder in said spring steel wire is composed of Fe and unavo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
JP S5644747 AHigh carbon steel wire rod with superior drawability—9
US 4,889,567 AHigh strength and high toughness steel bar, rod and wire and the process of producing the same198927
JP H0257637 AManufacture of spring with high fatigue strength and steel wire for spring for use therein—37
JP H1129839 ASpring steel with high toughness—10
JP 2000313937 ASteel wire rod, extra thin steel wire, and stranded steel wire—4
KR 20000071463 AHigh-carbon steel wire superior in resistance to longitudinal cracking, steel product for the same, and process for production of the same—3
JP 2000355736 AHigh carbon steel wire excellent in longitudinal cracking resistance, steel for high carbon steel wire and its production—15
EP 1,096,031 A2High-strength spring steel—7
EP 1,096,031 A3High-strength spring steel—1
JP 2001181794 AHigh strength spring steel—13
JP 2001240941 ABar wire rod for cold forging and its production method—35
US 6,322,641 B1High-carbon steel wire superior in resistance to longitudinal cracking, steel product for the same, and process for production of the same200147
US 6,406,565 B1High toughness spring steel200233
JP 2002180200 ASteel wire rod for hard-drawn spring, wire drawing rod for hard-drawn spring, hard-drawn spring and method for producing the hard-drawn spring—8
US 6,602,359 B1Bar or wire product for use in cold forging and method for producing the same200328
JP 2004002994 ASteel wire for hard drawn spring excellent in fatigue strength and set resistance, and hard drawn spring—10
US 2005173028 A1Steel wire for hard drawn spring excellent in fatigue strength and resistance to settling, and hard drawn spring—29
EP 1,577,411 A1Steel for spring being improved in quenching characteristics and resistance to pitting corrosion—11
US 7,074,282 B2Steel wire rod for hard drawn spring, drawn wire rod for hard drawn spring and hard drawn spring, and method for producing hard drawn spring200614
US 2009025832 A1Spring wire rod excelling in fatigue characteristics—3

Non-Patent Literature (2)

  • Extended European Search Report issued Mar. 22, 2011, in European Patent Application No. 07830847.5.
  • Office Action issued Apr. 7, 2011, in Korean Patent Application No. 10-2009-7008917 (with English-language translation).