A method for fabricating a dielectric layer structure includes providing a substrate, blanketly forming a low-k dielectric layer of an interlayer dielectric (ILD) layer, the low-k dielectric layer covering at least a first metal interconnect structure on the substrate, blanketly forming a single tensile film of the ILD layer having a thickness of 200-1500 angstroms on the low-k dielectric layer, and performing a moisture preventing treatment on the single tensile film. The single tensile layer possesses a stress comparative to a stress of the low-k dielectric layer and a hydrophobic characteristic that prevents itself from absorbing moisture.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a dielectric layer comprising steps of: providing a substrate; blanketly forming a low-k dielectric layer of an interlayer dielectric (ILD) layer, the low-k dielectric layer covering at least a first metal interconnect structure on the substrate; blanketly forming a single tensile film of the ILD layer having a thickness of 200-1500 angstroms on the low-k dielectric layer, the single tensile film comprising a tensile stress of about 50-100 MPa; and performing a moisture preventing treatment on the single tensile film.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the substrate further comprises at least a metal layer.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the low-k dielectric layer comprises porous low-k dielectric material or ultra low-k (ULK) dielectric material.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (32)

PatentTitleYearCitations
JP H06267935 AManufacture of semiconductor device—6
US 5,366,929 AMethod for making reliable selective via fills199444
US 5,387,546 AMethod for manufacturing a semiconductor device199598
US 6,010,943 AMethod of fabricating a cylindrical capacitor200017
US 6,015,759 ASurface modification of semiconductors using electromagnetic radiation200068
US 6,020,024 AMethod for forming high dielectric constant metal oxides2000398
US 6,121,164 AMethod for forming low compressive stress fluorinated ozone/TEOS oxide film200056
US 6,208,014 B1Use of multifunctional reagents for the surface modification of nanoporous silica films200175
US 2001023125 A1Interlayer insulating film forming method, semiconductor device and method of manufacturing the same—13
US 6,294,473 B1Method of polishing substrates comprising silicon dioxide and composition relating thereto200115
US 6,297,532 B1Semiconductor device and method of manufacturing the same200113
US 6,548,901 B1Cu/low-k BEOL with nonconcurrent hybrid dielectric interface200322
US 2005106762 A1Recovery of hydrophobicity of low-k and ultra low-k organosilicate films used as inter metal dielectrics—45
US 2005227488 A1Capping of copper structures in hydrophobic ILD using aqueous electro-less bath—7
US 2006043591 A1Low temperature process to produce low-K dielectrics with low stress by plasma-enhanced chemical vapor deposition (PECVD)—49
US 2006073650 A1Method to selectively strain NMOS devices using a cap poly layer—16
US 7,071,708 B2Chip-type sensor against ESD and stress damages and contamination interference20069
US 2006146099 A1Micro droplet control apparatus—22
US 2006170836 A1Electronic device, method for manufacturing electronic device, contact hole of electronic device, method for forming contact hole of electronic device—27
US 2007105297 A1Semiconductor devices and methods of manufacturing the same—44
US 2007114667 A1Alternate pad structures/passivation inegration schemes to reduce or eliminate IMC cracking in post wire bonded dies during Cu/Low-K BEOL processing—9
US 2007281497 A1Method to mitigate impact of uv and e-beam exposure on semiconductor device film properties by use of a bilayer film—30
US 2008020570 A1Dual damascene fabrication with low k materials—61
US 2008122045 A1Dual liner capping layer interconnect structure—14
US 7,381,451 B1Strain engineering—HDP thin film with tensile stress for FEOL and other applications200823
US 2008197513 A1Beol interconnect structures with improved resistance to stress—34
US 2009179003 A1Substrate processing method, substrate processing apparatus and recording medium—16
US 7,563,704 B2Method of forming an interconnect including a dielectric cap having a tensile stress200911

Non-Patent Literature (2)

  • Kohl et al. "Low k, Porous Methyl Silsesquioxane and Spin-On-Glass." Electrochemical and Solid-State Letters vol. 2 (1999): p. 77-79.
  • Wang et al."Dielectric Properties and Frequency Response of Self-Assembled Monolayers pf Alkanethiols", Langmuir, vol. 20, No. 12, 2004: pp. 5007-5012.