Patents
US 8,178,451 B2#33599947 Most CitedActiveUnited States (USPTO)Utility

Glass composition formulated for a glass-metal bond of a tube collector and glass-metal bond made with glass of said glass composition

3Forward Citations (#33599947 Global)
0.2/yrCitation Velocity (#32481510 Global)
1.02Citation PageRank (#40378863 Global)
20Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The glass-metal bond for a tube collector includes a glass tube and metal part bonded to the glass tube. In order to match the thermal expansion properties, the glass tube has the following composition: SiO 2 , 73-77 wt. %; B 2 O 3 , 6-<8 wt. %; Al 2 O 3 , 6-6.5 wt. %; Na 2 O, 5.5-7 wt. %; K 2 O, 1-3 wt. %; CaO, 0.5-3.2 wt. %; MgO, 0-2 wt. %; Fe 2 O 3 , 50-150 ppm; and TiO 2 0-<100 ppm. The ratio of the sum of the alkaline-earth metal oxides (in mol %) to the sum of the alkali metal oxides (in mol %) is ≦0.6. The metal part is preferably made of metal material no. 1.3981 according to DIN 17745. The glass composition itself is also part of the invention.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 3.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A glass-metal bond in a tube collector of a solar energy collection apparatus, said glass-metal bond comprising a glass tube and a metal component bonded to the glass tube, wherein said glass tube has a glass composition comprising: SiO 2 73-77 wt. % B 2 O 3 6-<8 wt. % Al 2 O 3 6-6.5 wt. % Na 2 O

  2. Claim 5Independent Claim

    5-7 wt. %

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
DE 4,430,710 C1Borsäurearmes Borosilikatglas und seine Verwendung199663
US 5,599,753 ABorosilicate glass weak in boric acid199773
EP 0,992,462 A1Borosilicate glass of high chemical resistance and its application—5
US 6,204,212 B1Borosilicate glass of greater resistance to chemical attack and applications thereof200134
DE 10,035,801 A1Borosilicatglas hoher chemischer Bestädigkeit und dessen Verwendungen—24
US 2003087745 A1Borosilicate glass with high chemical resistance and use thereof—33
US 6,794,323 B2Borosilicate glass with high chemical resistance and use thereof200442
DE 102004027120 A1Borosilicate glass for fluorescent lamp, consists of preset amount of oxides of silicon, boron, aluminum, lithium, sodium, potassium, magnesium, calcium, strontium, barium, zinc, zirconium, cerium, titanium, bismuth and molybdenum—19
US 2004266603 A1UV-radiation absorbing glass with high chemical resistance, especially for a fluorescent lamp, and methods of making and using same—32
DE 102004027119 A1Production of a UV-absorbed glass used in the production of gas discharge lamps, fluorescent lamps, xenon lamps, LCD displays, computer monitors and telephone displays comprises melting a raw material and producing a melt—25
US 2005037911 A1UV-radiation absorbing glass with reduced absorption of visible light and methods of making and using same—28
US 2005181925 A1Method of making a glass-metal joint, glass-metal joint made thereby and method of making a solar energy tube collector with said joint—23
DE 102004008559 A1Verwendung eines Glases für Glas-Metall-Verbindungen—13
DE 102006041469 B3Coating anti-reflection layer containing silicon dioxide on a borosilicate glass body comprises wetting the body containing e.g. silicon dioxide with a coating solution containing e.g. hydrochloric acid, followed by drying and annealing20087
US 2008057187 A1Method of making a wipe-resistant antireflection coating on a borosilicate glass body and coating solution for use in said method—11
US 7,375,043 B2UV-radiation absorbing glass with reduced absorption of visible light and methods of making and using same200825
US 2008128923 A1Glass for Semiconductor Encapsulation and Outer Tube for Semiconductor Encapsulation, and Semiconductor Electronic Parts—18
US 2008254301 A1Uv-radiation absorbing glass with reduced absorption of visible light and method of making and using same—20
US 7,491,668 B2UV-radiation absorbing glass with high chemical resistance, especially for a fluorescent lamp, and methods of making and using same200916
US 7,562,655 B2Method of making a glass-metal joint, glass-metal joint made thereby and method of making a solar energy tube collector with said joint200914

Non-Patent Literature (5)

  • DIN 12116: "Testing the Resistance of Glass to Attack by Boiling Hydrochloric Acid Solution, and Classification" Mar. 2001. Deutsche Norm, Ref. No. DIN 12116: 2001-03. ICS 81.040.10.
  • DIN 17745. Sep. 2002. Knetlegierungen Aus Nickel Und Eisen: Zusaivimensetzung, ICS 77.150.40, Ref. No. DIN 17745:2002-09.
  • ISO 695: "Glass-Resistance to Attack by a Boiling Aqueous Solution of Mixed Alkali-Method of Test and Classification" International Standard, Third Edition, 1891-05:15, Reference No. ISO 695:1991 (E).
  • ISO 719: "Glass-Hydrolytic Resistance of Glass Grains At 98 Degrees Celsius-Method of Test and Classification" International Standard, UDC 666.1 : 620.193.4, Ref. No. ISO 719-1985 (E). Second Edition, Oct. 1, 1985.
  • ISO 719: "Glass-Hydrolytic Resistance of Glass Grains At 98 Degrees Celsius—Method of Test and Classification" International Standard, UDC 666.1 : 620.193.4, Ref. No. ISO 719-1985 (E). Second Edition, Oct. 1, 1985.