Patents
US 8,169,090 B2#32912646 Most CitedActiveUnited States (USPTO)Utility

Encapsulating resin composition for preapplication, semiconductor device made with the same, and process for producing the same

3Forward Citations (#32912646 Global)
0.2/yrCitation Velocity (#32456541 Global)
1.07Citation PageRank (#37824890 Global)
18Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An encapsulation resin composition for preapplication, comprising (a) an epoxy resin, and (b) a curing agent having flux activity, wherein the tack after B-staging is at least 0 gf/5 mmφ and at most 5 gf/5 mmφ, and the melt viscosity at 130° C. is at least 0.01 Pa·s and at most 1.0 Pa·s; a preapplied encapsulated component and semiconductor device using the composition, and a process of fabrication thereof. The resin composition is less susceptible to air entrapment during provisional placement of semiconductor chips, and excels in workability and reliability.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An encapsulation resin composition for preapplication, comprising (a) an epoxy resin, and (b) a curing agent having flux activity, wherein the tack after B-staging is at least 0 gf/5 mmφ and at most 5 gf/5 mmφ, and the melt viscosity at 130° C. is at least 0.01 Pa·s and at most 1.0 Pa·s.

  2. Claim 2Depends on #1

    An encapsulation resin composition for preapplication in accordance with claim 1 , wherein the Tg after curing is at least 80° C. and at most 150° C.

  3. Claim 3Depends on #1

    An encapsulation resin composition for preapplication in accordance with claim 1 , further comprising (c) a solvent containing a first solvent that has good solubility for said epoxy resin and poor solubility for said curing agent.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
US 4,609,427 AMethod for producing ink jet recording head198688
US 4,719,255 AEpoxy resin composition for encapsulation of semi-conductor device198822
US 5,167,674 ABismaleimide-triazine resin bonded superabrasive wheels199225
US 5,248,757 AMesogenic cyanate functional maleimides and thermosets thereof19933
US 5,300,594 ABis(aminophenoxy)-alpha-substituted stilbenes, curable mixtures with epoxy resins and cured products199410
US 5,387,657 AEpoxy resins containing thiadiazole and/or oxadiazole moieties199537
US 5,442,039 AMesogenic polycyanates and thermosets thereof1995120
US 5,460,860 AMesogen-containing biaxially oriented films19958
US 5,470,946 AProducts resulting from polymerizing or curing polycyanates containing mesogenic moieties as lateral substituents19954
US 5,612,479 APolyphenols containing mesogenic moieties as lateral substituents19975
US 5,637,669 AEpoxy resins containing discotic mesogenic moieties199720
US 6,294,259 B1Polyimide hybrid adhesives200118
JP 2003212964 ALiquid sealing resin composition, method for assembling semiconductor element, and semiconductor device—12
JP 2003243449 AMethod of manufacturing semiconductor device and semiconductor device—16
JP 2004174574 ASolder paste and assembling method of semiconductor device using it—18
US 6,911,606 B2Electronic component for adhesion of a plurality of electrodes and method of mounting the same200512
US 6,919,420 B2Acid-cleavable acetal and ketal based epoxy oligomers200520
US 7,109,061 B2Wafer applied fluxing and underfill material, and layered electronic assemblies manufactured therewith200642

Non-Patent Literature (1)

  • Chinese Office Action issued on Jan. 29, 2010 for Chinese Application No. 200680025514.6 w/ English translation.