Polyethylene naphthalate fibers and method for producing the same
Abstract
Polyethylene naphthalate fibers that are characterized in that the fibers have a crystal volume of from 100 to 200 nm 3 obtained by wide angle X-ray diffraction of the fiber and a degree of crystallization of from 30 to 60%. It is preferred that the fibers have a maximum peak diffraction angle of wide angle X-ray diffraction of from 23.0 to 25.0°. The production method thereof is characterized in that a particular phosphorus compound is added to the polymer in a molten state, the spinning speed is from 4,000 to 8,000 m/min, and the molten polymer immediately after discharging from the spinneret is allowed to pass through a heated spinning chimney at a high temperature exceeding a temperature of the molten polymer by 50° C. or more, and is drawn.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Polyethylene naphthalate fibers comprising ethylene naphthalate as a major repeating unit, characterized in that the fibers have a crystal volume of from 100 to 200 nm 3 obtained by wide angle X-ray diffraction of the fiber and a degree of crystallization of from 30 to 60%.
- Claim 2Depends on #1
The polyethylene naphthalate fibers according to claim 1 , wherein the fibers have a maximum peak diffraction angle of wide angle X-ray diffraction of from 23.0 to 25.0°.
- Claim 3Depends on #1
The polyethylene naphthalate fibers according to claim 1 , wherein the fibers have an exothermic peak energy ΔHcd of from 15 to 50 J/g under a nitrogen stream and a temperature decreasing condition of 10° C. per minute.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗