Trench isolation structure having different stress
Abstract
By locally heating isolation trenches with different annealing conditions, a different magnitude of intrinsic stress may be obtained in different isolation trenches. In some illustrative embodiments, the different anneal temperature may be achieved on the basis of an appropriate mask layer, which may provide a patterned optical response for a lamp-based or laser-based anneal process. Consequently, the intrinsic stress of isolation trenches may be specifically adapted to the requirements of circuit elements, such as N-channel transistors and P-channel transistors.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method, comprising: forming a first isolation trench and a second isolation trench in a semiconductor layer, said first and second isolation trenches being filled with an insulating material; forming a mask layer to cover said first isolation trench and expose said second isolation trench; and heat treating said first and second isolation trenches by applying a heat generating radiation to said first and second isolation trenches in the presence of said mask layer to generate a first stress in said first isolation trench and a second stress in said second isolation trench different from said
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 12,408,323 B2 | Semiconductor memory device and method for manufacturing the same | 2025 | 0 |
References Cited — Backward Prior Art (11)
Non-Patent Literature (1)
- Ishibashi et al., "Novel Shallow Trench Isolation Process from Viewpoint of Total Strain Process Design for 45 nm Node Devices and Beyond," Japanese Journal of Applied Physics, 44:2153-56, 2005.