Patents
US 8,148,265 B2#27286082 Most CitedActiveUnited States (USPTO)Utility

Two-step hardmask fabrication methodology for silicon waveguides

4Forward Citations (#27286082 Global)
0.3/yrCitation Velocity (#26520509 Global)
1.05Citation PageRank (#38860114 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Techniques are disclosed for efficiently fabricating semiconductors including waveguide structures. In particular, a two-step hardmask technology is provided that enables a stable etch base within semiconductor processing environments, such as the CMOS fabrication environment. The process is two-step in that there is deposition of a two-layer hardmask, followed by a first photolithographic pattern, followed by a first silicon etch, then a second photolithographic pattern, and then a second silicon etch. The process can be used, for example, to form a waveguide structure having both ridge and channel configurations, or a waveguide (ridge and/or channel) and a salicide heater structure, all achieved using the same hardmask. The second photolithographic pattern allows for the formation of the lower electrical contacts to the waveguides (or other structures) without a complicated rework of the hardmask.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of making a silicon waveguide structure, the method comprising: depositing a hardmask layer on a substrate having a silicon layer on an oxide layer; etching the hardmask layer to provide a patterned hardmask defining patterns for a waveguide and at least one other structure; etching partway down the silicon layer with the patterned hardmask in place to form at least part of the waveguide and the at least one other structure; patterning a slab of the at least one other structure; and etching the remainder of the silicon layer down to the oxide layer with the patterned hardmask in place

  2. Claim 2Depends on #1

    The method of claim 1 wherein the hardmask layer includes a top layer that acts as a hardmask and a polish stop for chemical-mechanical

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,420,258 ADual input gyroscope198344
US 4,547,072 AOptical fiber gyro198533
US 4,748,617 AVery high-speed digital data bus1988113
US 4,921,354 AIdentical servo frequency modulated passive ring laser gyroscope199044
US 5,165,001 AGuided-wave optical branching device199270
WO 9,314,514 A1Vertical-cavity surface emitting laser optical interconnect technology—22
US 5,281,805 AOptical-input latch-circuit cell array199467
US 5,371,591 ATriaxial split-gain ring laser gyroscope199439
US 5,430,755 APressure-equalized self-compensating discharge configuration for triangular ring laser gyroscopes199531
US 5,625,636 AIntegration of photoactive and electroactive components with vertical cavity surface emitting lasers1997160
US 5,674,778 AMethod of manufacturing an optoelectronic circuit including heterojunction bipolar transistor, laser and photodetector199766
US 5,703,989 ASingle-mode waveguide structure for optoelectronic integrated circuits and method of making same1997109
EP 0,818,693 A1Optical waveguide device and manufacturing method of the same—16
US 5,736,461 ASelf-aligned cobalt silicide on MOS integrated circuits199899
US 5,828,476 ADual rate, burst mode, radiation hardened, optical transceiver199867
US 5,834,800 AHeterojunction bipolar transistor having mono crystalline SiGe intrinsic base and polycrystalline SiGe and Si extrinsic base regions199890
US 6,063,299 AManufacture of a silicon waveguide structure200039
US 6,117,771 AMethod for depositing cobalt200038
EP 1,067,409 A2Optical device having modified transmission characteristics by localized thermal treatment—19
WO 0,127,669 A1Cluster integration approach to optical transceiver arrays and fiber bundles—21
US 6,242,324 B1Method for fabricating singe crystal materials over CMOS devices2001189
US 6,306,722 B1Method for fabricating shallow trench isolation structure200151
US 6,331,445 B1Phototonic device with strain-induced three dimensional growth morphology200158
WO 0,216,986 A1Fiber-optic waveguides for transverse optical coupling—41
US 2002039830 A1Salicidation process for a fully depleted silicon-on-insulator device—11
US 6,387,720 B1Waveguide structures integrated with standard CMOS circuitry and methods for making the same200249

Non-Patent Literature (5)

  • "Erbium Doped Optical Waveguide Amplifiers on Silicon", P.G. KiK and A. Polman, MRS Bulletin 23(4), 48, Apr. 1998, 7 pages.
  • "Process Integration", Cobalt Self-aligned Silicide Process, Chapter 13.
  • Chao et al., "Analysis of Temperature Profiles of Thermo-optic Waveguides", Fiber and Integrated Optics, vol. 33.
  • Fijol et al., "Fabrication of Silicon-on-insulator Adiabatic Tapers for Low Loss Optical Interconnection of Photonic Devices".
  • Final Rejection from related U.S. Appl. No. 12/201,791, mailed Sep. 8, 2009.