Patents
US 8,147,609 B2#7883574 Most CitedActiveUnited States (USPTO)Utility

Non-dispersible concrete for underwater and underground construction

13Forward Citations (#7883574 Global)
0.9/yrCitation Velocity (#7712500 Global)
1.40Citation PageRank (#25548588 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A non-dispersible concrete for underwater and underground construction is disclosed, whose composition primarily comprises: coarse aggregate in a range of from 600 to 1200 kgw/m 3 ; fine aggregate 500 to 1100 kgw/m 3 , with a fineness modulus (F.M.) in a range of from 2.2 to 3.2; powder 300 to 700 kgw/m 3 ; mixing water 140 to 300 kgw/m 3 ; and cohesion-enhancing admixture (for example, polyacrylamide, PAA) whose solid content is 0.1 to 5.0 wt % of the powder. In addition, a SCC for underwater and underground construction is also developed and has excellent property of self-consolidation (its test value is 400 to 750 mm in slump flow spread test) and an appropriate compressive strength (between 14 to 70 MPa), so as can be widely applied to underwater and underground construction, whose composition further includes superplasticizer with solid content 0.1 to 3.0 wt % of the powder. Also, it covers: water to binder ratio (W/B) of 0.22 to 1.00, paste volume 0.25 to 0.60 m 3 , and water/powder volume ratio 0.5 to 2.95.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A self-consolidating concrete composition comprising: coarse aggregate in a range of from 600 to 1100 kgw/m 3 ; fine aggregate with a fineness modulus between 2.2 to 3.2, in a range of from 500 to 1100 kgw/m 3 ; powder containing at least cement, in a range of from 300 to 700 kgw/m 3 ; mixing water; cohesion-enhancing admixture; and superplasticizer; when the SCC composition is mixed, the water/cementitious material ratio is 0.22 to 1.00, paste volume 0.25 to 0.60 m 3 , and water to powder volume ratio 0.5 to 2.95; wherein the cohesion-enhancing admixture has a solid content of 0.1 to 5.0 wt %

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • JP 01051356 (Nakano et al.) Feb. 27, 1989 abstract only.
  • JP 01051356 (Nakano et al.) Feb. 27, 1989 Machine Translation in English.
  • JP 58190851 (Jobu) Nov. 7, 1983 abstract only.
  • JP 58190851 (Jobu) Nov. 7, 1983 Machine Translation in English.
  • JP 60239347 (Mori) Nov. 28, 1985 abstract only.