Process and device for producing strips of silicon steel or multiphase steel
Abstract
The invention relates to a method for producing strips ( 1 ) of steel, preferably of silicon steel, in particular of grain-oriented silicon steel or of multiphase steel in which a slab ( 3 ) is initially cast in a casting machine ( 2 ), wherein this is then rolled in at least one roll train ( 4, 5 ) to form strip ( 1 ) and wherein before and/or after the at least one roll train ( 4, 5 ), the slab is heated in at least one furnace ( 6, 7 ). In order to improve the quality and the scope for producing grain-oriented silicon steel or multiphase steel, the invention provides that the slab ( 3 ) is heated to a pre-rolling temperature (T 1 ) after the casting machine ( 2 ) and before a pre-roll train ( 4 ) in a first furnace ( 6 ), or the slab ( 3 ) enters into the pre-roll train ( 4 ) using the casting heat without the presence of the first furnace ( 6 ), the slab ( 3 ) is then rolled in the pre-roll train ( 4 ), the slab is then heated after the pre-roll train ( 4 ) in a second furnace ( 7 ) to a defined temperature (T 2 ) that is higher than the pre-rolling temperature (T 1 ), and then the slab ( 3 ) is rolled to the final strip thickness in a finish roll train ( 5 ).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing strips of silicon steel, comprising the steps of: casting a slab in a casting machine; hot-rolling the slab in a pre-roll train; heating the slab in a furnace after pre-rolling to a predetermined temperature in a range of 1,150° -1,350° C.; holding the slab at the predetermined temperature for a predetermined holding time until non-uniform distributions of alloying elements (segregation) are completely broken down; and thereafter, finish-rolling the slab to a predetermined slab thickness.
- Claim 2Depends on #1
The method according to claim 1 , comprising the step of heating the slab after casting to a pre-rolling temperature.
- Claim 3Depends on #1
The method according to claim 1 in which the slab-heating step includes heating the slab to a temperature from 1,150° -1,300° C. when the silicon steel, the slab i
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (2)
- Dr. J. von Schéele et al., Sauerstoff statt heisser Luft, Energy, v.1., 2003, pp. 18-19.
- Sten Ljungars et al. Erfolgreiche Umruestung von Durchlaufoefen auf Oxyfuel-Betrieb, Gaswaerme International, 2005, No. 3, pp. 193-194.