Patents
US 8,129,290 B2#3308809 Most CitedActiveUnited States (USPTO)Utility

Method to increase tensile stress of silicon nitride films using a post PECVD deposition UV cure

24Forward Citations (#3308809 Global)
1.7/yrCitation Velocity (#2781308 Global)
2.15Citation PageRank (#12920760 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

High tensile stress in a deposited layer such as silicon nitride, may be achieved utilizing one or more techniques, employed alone or in combination. High tensile stress may be achieved by forming a silicon-containing layer on a surface by exposing the surface to a silicon-containing precursor gas in the absence of a plasma, forming silicon nitride by exposing said silicon-containing layer to a nitrogen-containing plasma, and then repeating these steps to increase a thickness of the silicon nitride created thereby. High tensile stress may also be achieved by exposing a surface to a silicon-containing precursor gas in a first nitrogen-containing plasma, treating the material with a second nitrogen-containing plasma, and then repeating these steps to increase a thickness of the silicon nitride formed thereby. In another embodiment, tensile film stress is enhanced by deposition with porogens that are liberated upon subsequent exposure to UV radiation or plasma treatment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 24.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming silicon nitride, the method comprising: first, (i) disposing a substrate including a surface in a processing chamber; second, (ii) forming a silicon-containing layer on the surface by exposing the surface in the processing chamber to a silicon-containing precursor gas in the absence of a plasma; third, (iii) forming silicon nitride by exposing said silicon-containing layer in the processing chamber to a N 2 plasma; and repeating step (ii) and step (iii), in that order, wherein a vacuum purge of the processing chamber does not occur between step (ii) and step (iii), and the

  2. Claim 2Depends on #1

    The method of claim 1 wherein the N 2 plasma is formed from a gas mixture including molecular nitrogen.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Annex to Form PCT/ISA/206, Communication Relating to the Results of the Partial International Search, dated Feb. 21, 2008 for PCT application No. PCT/US2007/071387.
  • Banerjee et al., "Characterization of CVD Deposited Amorphous Fluorocarbons for Low k Interlayer Dielectrics", 1 Electrochem. Soc.. 146, 2219 (1999).
  • Charles, "Role of ions in SiO 2 deposition with pulsed and continuous helicon plasma", Pure and Applied Chemistry, 2002 -vol. 74, No. 3, pp. 401-405, 2002. IUPAC 401.
  • Cruden et al., "Thermal Decomposition of Low-k Pulsed Plasma Fluorocarbon Films. I. Effects of Precursors and Substrate Temperature", J. Electrochem. Soc. 146,4590 (1999).
  • Cruden et al., "Thermal Decomposition of Low-k Pulsed Plasma Fluorocarbon Films. II. Effect of Post-Deposition Annealing and Ambients", J. Electrochem. Soc. 146,4597 (1999).