Patents
US 8,129,015 B2#52266276 Most CitedActiveUnited States (USPTO)Utility

Modified moldable urethane with tunable haptics

1Forward Citations (#52266276 Global)
0.1/yrCitation Velocity (#50865374 Global)
0.83Citation PageRank (#52266276 Global)
33Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a slush moldable polymeric composition for forming a skin useable in interior trim components and methods of making the same. In at least one embodiment, the composition comprises a) from 50 to 99 wt. percent urethane elastomer, b) from 0.1 to 15 wt. percent propylene copolymer, c) from 0.1 to 25 wt. percent olefin modified thermoplastic, such as SEBS, and d) from 0.1 to 30 weight percent olefinic block copolymer, wherein the polymeric composition is slush moldable and vacuum formable. The modifiers include an olefin block copolymer (OBC) having a variable distribution of block lengths. The OBC is present in an amount from 0.1% to 30% of the total composition. The haptics of the polymeric composition is tunable by adjusting the amounts of the modifiers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A polymeric composition comprising: a) from 50 to 99 wt. percent urethane elastomer; b) from 0.1 to 15 wt. percent propylene copolymer; c) from 0.1 to 25 wt. percent olefin modified thermoplastic; and d) from 0.1 to 30 wt. percent olefinic block copolymer having a variable distribution of block lengths; wherein the polymeric composition is slush moldable and vacuum formable.

  2. Claim 2Depends on #1

    The composition of claim 1 , wherein the olefinic block copolymer is present in an amount from 5.0 to 12.5 wt. percent.

  3. Claim 3Depends on #1

    The composition of claim 1 , wherein the olefin modified thermoplastic comprises SEBS block copolymer present in an amount from 7.5 to 15 wt. percent and has a Shore A hardness of 50 to 60 and a density of 0.95 to 1.05 g/cm 3 .

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (33)

PatentTitleYearCitations
US 3,933,937 AMolding-grade polyurethane19769
US 5,824,738 ALight stable aliphatic thermoplastic urethane elastomers and method of making same199850
US 5,936,023 AMethod of manufacturing composite material of clay mineral and rubber199985
US 6,076,246 AMethod for manufacturing an automotive interior trim component and the resultant construction thereof200039
US 6,107,404 APaintable, surface-damage resistant reactor grade thermoplastic olefin (TPO)200016
EP 1,050,549 A2Aliphatic sinterable thermoplastic polyurethane molding compositions—10
US 6,166,139 APaintable, surface-damage resistant compounded grade thermoplastic olefin (TPO)200010
US 6,187,859 B1Light stable aliphatic thermoplastic urethane elastomers and method of making same200135
US 2001011784 A1Grafted and crosslinkable pulverulent thermoplastic polyolefin composition which has elasticity and flexibility properties—8
US 6,280,816 B1Method for manufacturing an automotive interior trim component and the resultant construction thereof20019
US 2002019487 A1Grafted and crosslinkable pulverulent thermoplastic polyolefin composition which has elasticity and flexibility properties—8
US 6,410,638 B1Aliphatic, sinterable, thermoplastic polyurethane molding compositions200226
US 6,409,493 B1Double-cast slush molding method and apparatus20026
US 2002095006 A1Surface properties in thermoplastic olefin alloys—5
US 6,524,509 B1Method for casting multicolored parts for automotive interior applications200317
US 6,632,525 B1Material and method for manufacturing plastic parts20036
US 6,709,619 B2Double-cast slush molding method20049
US 2005031870 A1Composite powder, preparation and use thereof—25
US 2006106147 A1Method for making nanocomposite materials—21
US 2006142531 A1Aliphatic sinterable thermoplastic polyurethanes and use thereof—15
US 2006173115 A1Nano-composite and compositions manufactured thereof—24
US 7,160,496 B2Thermoplastic compositions containing metal material20079
US 2007049720 A1Polyurethanes, their preparation and use—6
US 2007055005 A1Method for forming nanocomposite materials—3
WO 2008/077146 A1Double-cast slush molding compositions—3
US 2008182928 A1Polurethane powder lacquer—15
US 2008269419 A1Catalyst Composition Comprising Shuttling Agent For Tactic/ Atactic Multi-Block Copolymer Formation—6
US 2008269412 A1Catalytic Olefin Block Copolymers with Controlled Block Sequence Distribution—93
US 2008311812 A1Catalyst Composition Comprising Shuttling Agent for Higher Olefin Multi-Block Copolymer Formation—128

Non-Patent Literature (2)

  • European Search Report Dated Aug. 20, 2010, Application No. 10155182.8-2115, Applicant International Automotive Components Group North America, Inc., 7 Pages.
  • Leandro Pizzatto et al., "Synthesis and Characterization of Thermoplastic Polyurethane/Nanoclay Composites", Materials Science and Engineering C29 (2009), pp. 474-478.