Optical component for EUVL and smoothing method thereof
Abstract
The present invention provides a method for smoothing an optical surface of an optical component for EUVL. Specifically, the present invention provides a method for smoothing an optical surface of an optical component for EUVL made of a silica glass material containing TiO 2 and comprising SiO 2 as a main component with a laser having an oscillation wavelength, to which the optical component for EUVL has an absorption coefficient of 0.01 μm −1 or more, at a fluence of 0.3 to 1.5 J/cm 2 in an atmosphere having a water vapor partial pressure of 3.6 mmHg or less.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 2.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for smoothing an optical surface of an optical component for EUVL, comprising irradiating an optical surface having a concave defect of an optical component for EUV lithography (EUVL) made of a silica glass material containing TiO 2 and comprising SiO 2 as a main component with a laser having an oscillation wavelength, to which the optical component for EUVL has an absorption coefficient of 0.01 μm −1 or more, at a fluence of 0.3 to 1.5 J/cm 2 in an atmosphere having a water vapor partial pressure of 3.6 mmHg or less.
- Claim 2Depends on #1
The method according to claim 1 , comprising irradiating an optical surface having a concave defect with a depth of greater than 2 nm of the optical component for EUVL with a laser having an oscillation wavelength, to which the optical component for EUVL has the absorption coefficient of 0.0
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (5)
- "Specification for absorbing film stacks and multilayers on extreme ultraviolet lithography mask blanks", SEMI, P38-1102, 2002, pp. 1-8.
- "Specification for extreme ultraviolet lithography mask blank", SEMI, P37-1102, 2002, pp. 1-10.
- Alan Stivers, et al., "Evaluation of the Capability of a Multibeam Confocal Ins System for Inspection of EUVL Mask Blanks", Proceedings of SPIE, vol. 4889, 2002, pp. 408-417.
- Hiroshi Sawada, et al., "Mirror Finishing Using Laser-Induced Periodic Surface Structures", Journal of the Japan Society for Precision Engineering, vol. 73, No. 10, Oct. 5, 2007, pp. 1159-1163 (with partial English translation).
- Kiwamu Takehisa, et al.; "EUV Mask Substrate Flatness Improvement by Laser Irradiation"; Proc. of SPIE, Photomask Technology, 2007, vol. 6730, pp. 673051-1-673051-5.