Patents
US 8,124,264 B2#73404139 Most CitedActiveUnited States (USPTO)Utility

Ion-conductive material and use thereof

0Forward Citations (#73404139 Global)
0.0/yrCitation Velocity (#73404139 Global)
0.56Citation PageRank (#73404139 Global)
23Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Disclosed is an ion-conductive material which comprises an ionic liquid and can realize a higher level of safety. Also disclosed is an electrochemical device using the ion-conductive material. Further disclosed is a method for manufacturing an electrochemical device. An ion-conductive material comprising an ionic liquid satisfying the following conditions: the ionic liquid comprises two or more types of anion, such that at least one type thereof is an anion having a structure in which one or more electron-withdrawing groups are bonded to a central atom having one more non-covalent electron pairs; and the ionic liquid has a maximum exothermic heat-flow peak height no greater than 2 W/g as measured by DSC (measurement temperature range: ordinary temperature to 500° C., rate of temperature rise: 2° C./minute). Preferably, the ion-conductive material comprises an ionic liquid having a gross calorific value of no greater than 1000 J/g as measured by the DSC.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An ionic liquid satisfying the following conditions: (a) the ionic liquid comprises 1-ethyl-3-methyl imidazolium bis-trifluoromethylsulfonylimide (EMI-TSFI) and 1-ethyl-3-methyl imidazolium bis(perfluoroethylsulfonyl)imide (EMI-BETI) and satisfies the condition: (EMI-BETI)/{(EMI-TFSI)+(EMI-BETI)}≧10 mol %, or comprises EMI-TFSI and 1-ethyl-3-methyl imidazolium tetrafluoroborate (EMI-BF 4 ) and satisfies the condition: (EMI-BF 4 )/{(EMI-TFSI)+(EMI-BF 4 )}≧40 mol %; and (b) the ionic liquid has a maximum exothermic heat-flow peak height no greater than 2 W/g as measured by DSC, where a measureme

  2. Claim 2Depends on #1

    The ionic liquid according to claim 1 , wherein the ionic liquid has a gross caloric value of no greater than 1000

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
US 5,683,832 AHydrophobic liquid salts, the preparation thereof and their appliction in electrochemistry1997127
US 5,827,602 AHydrophobic ionic liquids1998432
JP H11307123 ALithium secondary battery and electrolyte thereof and electric equipment—40
US 6,063,522 AElectrolytes containing mixed fluorochemical/hydrocarbon imide and methide salts200088
US 6,210,835 B1Lithium secondary battery and liquid electrolyte for the battery200167
US 2001010877 A1Electrical appliance using lithium secondary batteries—23
US 6,350,545 B2Sulfonylimide compounds200220
US 6,531,241 B1Cyclic delocalized cations connected by spacer groups200345
US 2003211389 A1Guanidine derivatives as cations for ambient temperature molten salts in electrochemical power sources—24
JP 2003331918 ACold melting salt, and lithium secondary cell using the same—62
WO 03,106,419 A1Room-temperature molten salt, process for producing the same and applications thereof—31
US 2004038127 A1Small cation/delocalizing anion as an ambient temperature molten salt in electrochemical power sources—10
JP 2004155765 ASmall cation/delocalized anion as ambient temperature-molten salt in electrochemical electric source—3
JP 2004253357 AGuanidine derivative as cation for normal temperature molten salt in electrochemical power supply—5
JP 2005104846 AQuaternary ammonium ambient-temperature molten salt and its manufacturing method—9
JP 2005104845 AQuaternary ammonium ambient-temperature molten salt and manufacturing method—18
JP 2005139100 AOrdinary temperature melted salt—27
JP 2005183195 ALithium secondary battery—29
US 2005158623 A1Nonaqueous electrolyte for electrochemical devices—28
US 2005175867 A1Room-temperature molten salt, process for producing the same and applications thereof—36
JP 2005229103 ANonaqueous electrolyte for electrochemical element, and electric double-layer capacitor or secondary cell containing the same—30
JP 2006190618 AIonic liquid composition and electrochemical device containing same—11
US 7,582,380 B1Lithium-ion cell with a wide operating temperature range200918

Non-Patent Literature (5)

  • International Search Report, dated Nov. 28, 2006.
  • Korean Office Action for Korean Patent App. No. 10-2008-7007180, dated Feb. 25, 2010.
  • Machine translation of JP 2005/139100, Jun. 2005.
  • Machine translation of JP 2006/190618, Jul. 2006.
  • Notification of Reasons for Rejection for JP Appl. No. 2005-245897 dated Apr. 27, 2010.