Sintered refactory material based on silicon carbide with a silicon nitride binder
Abstract
A sintered material based on silicon carbide (SiC) reactively sintered between 1,100° C. and 1,700° C. to form a silicon nitride binder (Si 3 N 4 ), intended in particular for fabricating an aluminum electrolysis cell, including 0.05% to 1.5% of boron, the Si 3 N 4 /SiC weight ratio being in the range 0.05 to 0.45.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A sintered material based on silicon carbide (SiC) reactively sintered between 1,100° C. and 1,700° C. to form a silicon nitride (Si 3 N 4 ) binder, including a boron compound, the boron compound being selected from the group consisting of oxides, carbides, nitrides, fluorides containing boron and CaB 6 , a percentage by weight of boron being in a range of 0.05% to 1.5%, and a Si 3 N 4 /SiC weight ratio being in a range 0.05 to 0.45, a porosity of the sintered material being 10% or more.
- Claim 2Depends on #1
The sintered material according to claim 1 , in which the percentage by weight of boron is in the range 0.05% to 1.2%.
- Claim 3Depends on #1
The sintered material according to claim 1 , in which the Si 3 N 4 /SiC weight ratio is in the range 0.1 to 0.2.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (3)
- Derwent abstract of JP 58091070, May 1983.
- International Search Report, dated Jun. 5, 2009.
- Notification of the Second Office Action dated Mar. 1, 2010.