Integrated BEOL thin film resistor
Abstract
In the course of forming a resistor in the back end of an integrated circuit, an intermediate dielectric layer is deposited and a trench etched through it and into a lower dielectric layer by a controllable amount, so that the top of a resistor layer deposited in the trench is close in height to the top of the lower dielectric layer; the trench is filled and the resistor layer outside the trench is removed, after which a second dielectric layer is deposited. Vias passing through the second dielectric layer to contact the resistor then have the same depth as vias contacting metal interconnects in the lower dielectric layer. A tri-layer resistor structure is employed in which the resistive film is sandwiched between two protective layers that block diffusion between the resistor and BEOL ILD layers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A resistive structure comprising: a first dielectric layer; a trench formed in said first dielectric layer; a liner of resistive material conformably disposed in said trench; a second dielectric material conformably disposed on said liner and filling said trench; a first terminal coupled to said liner; and a second terminal coupled to said liner and offset from the first terminal to achieve a defined resistance level between the terminals.
- Claim 2Depends on #1
A resistive structure according to claim 1 , wherein said trench extends through said first dielectric layer and extends a controllable depth into a third dielectric layer below said first dielectric layer.
- Claim 3Depends on #1
A resistive structure according to claim 1 , wherein said liner comprises: a first protective layer; a layer of resistive material conformably disposed on said lower protective layer
Technical Overview & Description