Patents
US 8,093,154 B2#13285465 Most CitedExpiredUnited States (USPTO)Utility

Etchant treatment processes for substrate surfaces and chamber surfaces

8Forward Citations (#13285465 Global)
0.6/yrCitation Velocity (#13872408 Global)
1.90Citation PageRank (#15755905 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In one embodiment of the invention, a method for finishing or treating a silicon-containing surface is provided which includes removing contaminants and/or smoothing the surface contained on the surface by a slow etch process (e.g., about <100 Å/min). The silicon-containing surface is exposed to an etching gas that contains an etchant and a silicon source. Preferably, the etchant is chlorine gas so that a relatively low temperature (e.g., <800° C.) is used during the process. In another embodiment, a method for etching a silicon-containing surface during a fast etch process (e.g., about >100 Å/min) is provided which includes removing silicon-containing material to form a recess in a source/drain (S/D) area on the substrate. In another embodiment, a method for cleaning a process chamber is provided which includes exposing the interior surfaces with a chamber clean gas that contains an etchant and a silicon source. The chamber clean process limits the etching of quartz and metal surfaces within the process chamber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a silicon-containing material on a substrate surface, comprising: positioning a substrate comprising a silicon material containing a contaminant within a process chamber; exposing the substrate to an etching gas comprising chlorine gas and a silicon source at a temperature of less than about 800° C. during an etching process to remove the contaminant; exposing the substrate to a deposition gas during a deposition process; and exposing the process chamber to a chamber clean gas comprising the chlorine gas and the silicon source during a chamber clean process.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the substrate is removed from the process chamber prior to starting the chamber clean process.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the silicon source comprises a reagent selected from the group consisting of silane, disilane,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,663,831 AMethod of forming transistors with poly-sidewall contacts utilizing deposition of polycrystalline and insulating layers combined with selective etching and oxidation of said layers1987151
US 4,834,831 AMethod for growing single crystal thin films of element semiconductor1989255
US 5,028,560 AMethod for forming a thin layer on a semiconductor substrate199169
US 5,112,439 AMethod for selectively depositing material on substrates1992134
US 5,129,958 ACleaning method for semiconductor wafer processing apparatus1992125
US 5,273,930 AMethod of forming a non-selective silicon-germanium epitaxial film1993126
US 5,288,658 AProcess for the formation of an amorphous silicon deposited film with intermittent irradiation of inert gas plasma199460
US 5,294,286 AProcess for forming a thin film of silicon1994295
US 5,308,788 ATemperature controlled process for the epitaxial growth of a film of material199453
US 5,372,860 ASilicon device production199463
US 5,374,570 AMethod of manufacturing active matrix display device using insulation layer formed by the ale method1994213
US 5,469,806 AMethod for epitaxial growth of semiconductor crystal by using halogenide199554
US 5,480,818 AMethod for forming a film and method for manufacturing a thin film transistor1996348
US 5,503,875 AFilm forming method wherein a partial pressure of a reaction byproduct in a processing container is reduced temporarily1996216
US 5,521,126 AMethod of fabricating semiconductor devices1996141
US 5,527,733 AImpurity doping method with adsorbed diffusion source199684
US 5,674,304 AMethod of heat-treating a glass substrate1997192
US 5,693,139 AGrowth of doped semiconductor monolayers1997163
US 5,796,116 AThin-film semiconductor device including a semiconductor film with high field-effect mobility1998194
US 5,807,792 AUniform distribution of reactants in a device layer1998149
US 5,906,680 AMethod and apparatus for low temperature, low pressure chemical vapor deposition of epitaxial silicon layers1999105
US 5,908,307 AFabrication method for reduced-dimension FET devices1999111