Patents
US 8,092,861 B2#89601034 Most CitedActiveUnited States (USPTO)Utility

Method of fabricating an ultra dielectric constant (K) dielectric layer

0Forward Citations (#89601034 Global)
0.0/yrCitation Velocity (#89601034 Global)
0.56Citation PageRank (#89601034 Global)
30Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A fabrication method of an ultra low-k dielectric layer is provided. A deposition process is performed, under the control of a temperature varying program or a pressure varying program, by reacting a dielectric matrix to form porous low-k dielectric layers with a gradient density on a barrier layer over a substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating an ultra low dielectric constant (k) dielectric layer, the method comprising: performing a deposition process with a dielectric matrix and a porogen, wherein the deposition process is controlled by a temperature varying program for the dielectric matrix and the porogen to react to form a plurality of porous low-k dielectric layers stacked on a dielectric barrier layer above a substrate; wherein the temperature varying program is a gradient temperature varying program comprising a plurality of temperature steps, the stacked porous low-k dielectric layers are formed by th

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the gradient temperature varying p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (30)

PatentTitleYearCitations
US 6,080,640 AMetal attachment method and structure for attaching substrates at low temperatures2000239
US 6,187,692 B1Method for forming an insulating film20012
US 6,465,372 B1Surface treatment of C-doped SiO2 film to enhance film stability during O2 ashing200267
US 6,531,412 B2Method for low temperature chemical vapor deposition of low-k films using selected cyclosiloxane and ozone gases for semiconductor applications200334
US 6,583,046 B1Post-treatment of low-k dielectric for prevention of photoresist poisoning200367
US 6,593,043 B2Composition of positive photosensitive resin precursor, and display device thereof200322
US 2003211244 A1Reacting an organosilicon compound with an oxidizing gas to form an ultra low k dielectric—29
US 2004126929 A1Silicon carbide having low dielectric constant—27
US 6,784,101 B1Formation of high-k gate dielectric layers for MOS devices fabricated on strained lattice semiconductor substrates with minimized stress relaxation200477
US 6,798,043 B2Structure and method for isolating porous low-k dielectric films200422
US 6,805,139 B1Systems and methods for photoresist strip and residue treatment in integrated circuit manufacturing200491
US 2005048795 A1Method for ultra low-K dielectric deposition—40
US 6,905,981 B1Low-k dielectric materials and processes20055
US 6,919,101 B2Method to deposit an impermeable film on porous low-k dielectric film20057
US 2005255710 A1Porous materials—16
CN 1,716,546 ADielectric layer, its forming method and integrated circuit with the same—3
TW 200,610,054 ALow temperature process to produce low-k dielectrics with low stress by plasma-enhanced chemical vapor deposition (PECVD)—1
US 7,015,581 B2Low-K dielectric material system for IC application200619
US 7,084,079 B2Method for low temperature chemical vapor deposition of low-k films using selected cyclosiloxane and ozone gases for semiconductor applications200622
US 7,087,982 B2Nitrogen-containing polymers as porogens in the preparation of highly porous, low dielectric constant materials20068
US 7,125,790 B2Inclusion of low-k dielectric material between bit lines20067
US 7,125,794 B2Method of manufacturing semiconductor device20063
US 7,138,333 B2Process for sealing plasma-damaged, porous low-k materials20069
US 7,176,144 B1Plasma detemplating and silanol capping of porous dielectric films200731
US 2007173071 A1SiCOH dielectric—34
US 2007173070 A1Porous low-k dielectric film and fabrication method thereof—4
TW 200,729,395 APorous low-k dielectric film and fabrication method thereof—1
JP 2007258403 APorous low dielectric constant thin film and its manufacturing method—4
US 2009280637 A1Method of manufacturing semiconductor device including ultra low dielectric constant layer—10
US 7,723,237 B2Method for selective removal of damaged multi-stack bilayer films20108

Non-Patent Literature (5)

  • Kim, Suhan, et al., "Effect of Pore Generating Materials on the Electrical and Mechanical Properties of Porous Low-k Films". Macromolecular Research, vol. 15, No. 1, Feb. 28, 2007, pp. 1-4.
  • Kuo, Ming-Shu, et al., "Surface and near-surface modifications of ultralow dielectric constant materials exposed to plasmas under sidewall-like conditions". J. Vac. Sci. Technol. B 28(6), Nov./Dec. 2010, pp. 1104-1110.
  • Park, S.J., et al., "Formation of nanoporous organosilicate films using cyclodextrins as a porogen". Current Applied Physics 6 (2006) 743-746.
  • Rajagopalan, T., et al., "Supercritical carbon dioxide extraction of porogens for the preparation of ultralow-dielectric-constant films". Applied Physics Letters, vol. 82, No. 24, Jun. 16, 2003, pp. 4328-4330.
  • Yang, G.Y. et al., "Nanoporous Ultra-Low Dielectric Constant Materials". NISCT Center for Neutron Research Scientific Highlights, May 2002, no page numbers.