Patents
US 8,088,947 B2#37217830 Most CitedActiveUnited States (USPTO)Utility

Method for producing methacrolein and/or methacrylic acid

2Forward Citations (#37217830 Global)
0.1/yrCitation Velocity (#39629472 Global)
1.12Citation PageRank (#35733218 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a method for producing methacrolein and/or methacrylic acid characterized in that the catalyst filling length of a dehydration catalyst layer is 3 to 20% of the catalyst filling length of an oxidation catalyst layer in a method where raw material gas containing gaseous t-butanol is supplied to a fixed-bed multitubular reactor having a dehydration catalyst layer and an oxidation catalyst layer in this order, from the entrance for raw material gas toward the exit, to produce methacrolein and/or methacrylic acid by dehydration reaction and catalytic gas phase oxidation reaction, and the present invention can increase the conventional yield of approximately 80% to 81 to 82% even when a reaction bath temperature is relatively low (approximately 355° C.).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing methacrolein and/or methacrylic acid, wherein tertiary butanol, a raw material, is supplied to a fixed-bed multitubular reactor with a dehydration catalyst layer and an oxidation catalyst layer for dehydration to obtain water and isobutylene and the isobutylene is oxidized to produce methacrolein and/or methacrylic acid, and characterized in that the filling length of catalyst in the dehydration catalyst layer which is contacted by tertiary butanol before supplying the tertiary butanol to the oxidation catalyst layer is 3 to 20% of the filling length of catalyst in the o

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein a dehydration catalyst is alumina or alumina-silica.

  3. Claim 3Depends on #1, #2

    The method according to claim 1 or claim 2 , wherein a temperature of the dehydration catalyst layer is 250 to 400° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗