Abstract
The present invention provides high strength thick welded steel pipe for line pipe superior in low temperature toughness, and a method of production of the same. A base material steel plate containing C: 0.010 to 0.050%, Si: 0.01 to 0.50%, Mn: 0.50 to 2.00%, Al: 0.020% or less, Ti: 0.003 to 0.030%, and Mo: 0.10 to 1.50%, having a carbon equivalent Ceq of 0.30 to 0.53, having a crack susceptability parameter Pcm of 0.10 to 0.20, satisfying formula 3, comprised an area ratio of 20% or less of polygonal ferrite and an area ratio of 80% or more of bainite, and having an effective crystal grain size of 20 μm or less is formed into a pipe shape, then seam welded to make the effective crystal grain size of the heat affected zone 150 μm or less: 10C+100Al+5Mo+5Ni<3.3 formula 3.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
High strength thick line pipe use welded steel pipe, superior in low temperature toughness, the welded steel pipe comprising steel pipe obtained by seam welding a base material steel plate formed into a pipe shape, wherein said base material steel plate comprises, by mass %: C: 0.010 to 0.050%, Si: 0.01 to 0.50%, Mn: 0.50 to 2.00%, S: 0.0001 to 0.0050%, Ti: 0.003 to 0.030%, Mo: 0.10 to 1.50%, B: 0.0003 to 0.0030%, O: 0.0001 to 0.0080%, and a balance of iron and unavoidable impurities, wherein P and Al are present at most as impurities, wherein P is limited to 0.050% or less, and Al is limited
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (26)
Non-Patent Literature (2)
- Extended European Search Report dated Jun. 1, 2011 issued in corresponding EPO Application No. EP 07 85 0314.
- International Search Report dated Mar. 18, 2008 issued in corresponding PCT Application No. PCT/JP2007/073740.