Abstract

Formulations and methods of making solar cells are disclosed. In general, the invention provides a solar cell comprising a contact made from a mixture wherein, prior to firing, the mixture comprises at least one aluminum source, at least one boron source, and about 0.1 to about 10 wt % of a glass component. Within the mixture, the overall content of aluminum is about 50 wt % to about 85 wt % of the mixture, and the overall content of boron is about 0.05 to about 20 wt % of the mixture.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 45 · Forward citations: 7.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A solar cell comprising two separate layers, a silicon layer and a contact layer deposited over a surface of the silicon layer and made from a mixture, wherein, prior to firing, the mixture comprises: a. at least one aluminum source, b. at least one boron source, and c. about 0.1 to about 10 wt % of a glass component, wherein the glass component is devoid of intentionally added lead in any form, and wherein the glass component comprises: (i) about 12 to about 50 mole % Bi 2 O 3 , (ii) about 25 to about 65 mole % SiO 2 , (iii) about 5 to about 15 mole % B 2 O 3 , and (iv) about 4 to about 26 mo

  2. Claim 2Depends on #1

    The solar cell of claim 1 wherein the aluminum source is selected from the g

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (45)

PatentTitleYearCitations
US 3,900,945 AOrganic semiconductor solar cell197543
US 4,070,517 ALow fired conductive compositions197839
US 4,088,502 ACorrosion resistant castable refractory mix197834
US 4,163,678 ASolar cell with improved N-region contact and method of forming the same197942
US 4,235,644 AThick film silver metallizations for silicon solar cells198063
US 4,703,553 ADrive through doping process for manufacturing low back surface recombination solar cells198786
US 4,899,704 ASelf-lubricating bearing19908
US 5,074,920 APhotovoltaic cells with improved thermal stability199141
US 5,178,685 AMethod for forming solar cell contacts and interconnecting solar cells1993245
US 5,468,652 AMethod of making a back contacted solar cell1995272
US 5,584,941 ASolar cell and production process therefor199643
US 5,922,627 ALow resistivity palladium-silver compositions199915
US 5,928,438 AStructure and fabrication process for self-aligned locally deep-diffused emitter (SALDE) solar cell1999203
US 5,942,048 APhotovoltaic element electrode structure thereof and process for producing the same1999124
US 6,069,065 ASemiconductor device fabrication method200035
US 6,071,753 AMethod of producing a solar cell200043
US 6,093,882 AMethod of producing a solar cell; a solar cell and a method of producing a semiconductor device200080
US 6,096,968 ASolar cell with a back-surface field2000102
US 6,262,359 B1Aluminum alloy back junction solar cell and a process for fabrication thereof2001125
US 6,402,839 B1System for stabilizing dendritic web crystal growth20028
US 6,469,243 B2Dye-sensitizing solar cell, method for manufacturing dye-sensitizing solar cell and solar cell module200263
US 6,576,391 B1Photosensitive paste a plasma display, and a method for the production thereof200328
US 2003154592 A1Method to embed thick film components—42

Non-Patent Literature (3)

  • Greenhunt, "Effects of composition, processing, and structure on properties of ceramics and glasses", ASM Handbooks, 2002.
  • KB Alloys product listing from Jan. 2004, www.kballoys.com, obtained from www.web.archive.org.
  • Krause, et al., Determination of Aluminum Diffusion Parameters in Silicon, Journal of Applied Physics 91, May 1, 2002.