Abstract

High density oxide films are deposited by a pulsed-DC, biased, reactive sputtering process from a titanium containing target to form high quality titanium containing oxide films. A method of forming a titanium based layer or film according to the present invention includes depositing a layer of titanium containing oxide by pulsed-DC, biased reactive sputtering process on a substrate. In some embodiments, the layer is TiO 2 . In some embodiments, the layer is a sub-oxide of Titanium. In some embodiments, the layer is Ti x O y wherein x is between about 1 and about 4 and y is between about 1 and about 7. In some embodiments, the layer can be doped with one or more rare-earth ions. Such layers are useful in energy and charge storage, and energy conversion technologies.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A titanium-based layer, comprising: titanium, the amount of titanium in the layer being represented by Ti x , where x is between about 1 and about 4; and oxygen, the amount of oxygen in the layer being represented by O y , where y is between about 1 and about 7, wherein: the titanium-based layer is densified, has a uniform thickness, is substantially free from columnar structures, and has a figure of merit, defined as the product of a dielectric constant of the titanium-based layer and a breakdown voltage of the titanium based layer, greater than 200 through a deposition process using a pulsed

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,309,302 AMethod of preparing an electron tube including sputtering a suboxide of titanium on dielectric components thereof196762
US 3,616,403 APrevention of inversion of p-type semiconductor material during rf sputtering of quartz197153
US 3,850,604 APreparation of chalcogenide glass sputtering targets197459
US 4,006,070 AMetal oxide films197737
US 4,082,569 ASolar cell collector197857
US 4,099,091 AElectroluminescent panel including an electrically conductive layer between two electroluminescent layers197829
US 4,111,523 AThin film optical waveguide197854
US 4,437,966 ASputtering cathode apparatus1984100
US 4,587,225 AHigh-strength zirconia type sintered body1986131
US RE32449 ECeramic body of zirconium dioxide (ZrO2) and method for its preparation1987107
US 4,915,810 ATarget source for ion beam sputter deposition199073
US 4,978,437 AMethod of applying optical coatings of silicon compounds by cathode sputtering, and a sputtering cathode for the practice of the method199064
US 5,085,904 ABarrier materials useful for packaging1992163
US 5,110,696 ARechargeable lithiated thin film intercalation electrode battery199296
US 5,119,460 AErbium-doped planar optical device199290
US 5,173,271 AEnhanced radiative zone-melting recrystallization method and apparatus199222
US 5,174,876 AMethod of making an optical component by ion implantation199228
US 5,200,029 AMethod of making a planar optical amplifier199344
US 5,225,288 ASolvent blockers and multilayer barrier coatings for thin films199333
US 5,237,439 APlastic-substrate liquid crystal display device with a hard coat containing boron or a buffer layer made of titanium oxide199379
US 5,296,089 AEnhanced radiative zone-melting recrystallization method and apparatus199433
US 5,338,625 AThin film battery and method for making same1994635
US 5,355,089 AMoisture barrier for battery with electrochemical tester199477