Patents
US 8,075,710 B2#27300407 Most CitedActiveUnited States (USPTO)Utility

Soft magnetic composite materials

4Forward Citations (#27300407 Global)
0.3/yrCitation Velocity (#27810226 Global)
1.05Citation PageRank (#39085598 Global)
30Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for the manufacture of soft magnetic composite components is provided including the steps of: die compacting a powder composition including a mixture of soft magnetic, iron or iron-based powder, core particles of which are surrounded by an electrically insulating, inorganic coating, and an organic lubricant in an amount of 0.05 to 1.5% by weight of the composition, the organic lubricant being free from metal and having a temperature of vaporization less than the decomposition temperature of the coating; ejecting the compacted body from the die; heating the compacted body in an inert atmosphere to a temperature above the vaporization temperature of the lubricant and below the decomposition temperature of the inorganic coating for removing the lubricant from the compacted body, and subjecting the body obtained after heating the compacted body in an inert atmosphere to heat treatment at a temperature between 300 and 600 in water vapor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the manufacture of soft magnetic composite components comprising the steps of: die compacting a powder composition comprising a mixture of soft magnetic, iron or iron-based powder, core particles of which are surrounded by an electrically insulating, inorganic coating, and an organic lubricant in an amount of 0.05 to 1.5% by weight of the composition, said organic lubricant being free from metal and having a temperature of vaporisation less than the decomposition temperature of the coating; ejecting the compacted body from the die; heating the compacted body in an inert atmospher

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (30)

PatentTitleYearCitations
JP S5143007 ARusubandenwahoshiki—12
JP S54150307 AManufacture of ferriferous sintered part—4
SU 863,178 A1Method of producing magnetically soft iron19812
JP S57114637 ASoft magnetic material and its manufacture—9
SU 1,734,946 A1Method to obtain iron-based magnetically soft materials19922
JP H07166202 ALow aspect ratio flat soft magnetic metal powder and production thereof—8
RU 2,040,810 C1Method for producing nonretentive material199513
JP H07245209 ADust core and its manufacturing method—30
WO 9,730,810 A1Phosphate coated iron powder and method for the manufacturing thereof—16
US 5,770,136 AMethod for consolidating powdered materials to near net shape and full density199848
WO 9,903,622 A1Process for preparation of soft magnetic composites and the composites prepared—13
CN 1,211,943 APhosphate coated iron powder and method for manufacturing thereof—8
JP 2000178603 AStabilizing method of weight of green compact in powder molding process of sintered parts—4
WO 0,140,416 A1Lubricant combination and process for the preparation thereof—5
JP 2001510286 A軟磁性合成材およびその製造方法—7
CN 1,322,366 AMouldable material and method for producing weakly magnetic composite material therewith—1
JP 2001342478 ALubricating agent for lubrication of mold and method for manufacturing high density molded article of iron based powder—24
US 6,348,265 B1Phosphate coated iron powder and method for the manufacturing thereof200267
US 6,419,877 B1Compressed soft magnetic materials200212
US 6,485,579 B1Process for preparation of soft magnetic composites and the composites prepared200228
JP 2003515661 A潤滑剤複合物及びその製造方法—7
US 6,562,458 B2Iron powder and method for the preparation thereof200319
US 2004007291 A1Magnetic core insulation—9
US 6,706,206 B1Mouldable material and method for producing a weakly magnetic composite material therewith200412
WO 2004/037468 A1Method of preparing iron-based components by compaction with elevated pressures—4
WO 2004/038740 A1Heat treatment of soft magnetic components—5

Non-Patent Literature (3)

  • Decision on Grant issued by Federal Service on Industrial Property, Patents and Trade Marks for Application No. 2008101535, Nov. 9, 2009, Moscow, Russia.
  • English Translation of Decision on Grant issued by Federal Service on Industrial Property, Patents and Trade Marks for Application No. 2008101535, Nov. 9, 2009, Moscow, Russia.
  • English-language translation of JPO Office Action mailed on Nov. 9, 2010, in corresponding Japanese Patent Application No. JP 2008-516788.