Low cost high strength martensitic stainless steel
Abstract
A cobalt-free low cost high strength martensitic stainless steel, with concentration of Ni up to 3.0% and Mo up to 1.0% of weight, has HRC of 53, UTS of 297 ksi, YS of 220 ksi, Charpy V-notch impact energy of 17.8 ft-lb, corrosion resistance in salt spray test ASTM 117. The steel was melted in an open induction furnace and vacuum arc remelting (VAR) and/or electroslag remelting (ESR) were not used to refine the steel. Further processing included homogenized annealing, hot rolling, and recrystallization annealing. The steel was heat treated by oil quenching, refrigeration, and low tempering. The steel has a microstructure consisting essentially of small packets of fine martensite laths, retained austenite, and carbides as centers of growth of the martensite laths. The cost and energy in making the steel are substantially reduced.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 9.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A martensitic steel comprising by weight: about 0.3% to 0.65% of C; about 7.5% to 12.5.0% of Cr; about 0.1% to 1.0% of Mo; about 0.1% to 3.0% of Ni; about 0.3% to 1.5% of Mn; at least one element selected from the group consisting of Si, Sn, and Ge wherein (Si+Sn+Ge) is about 0.1% to 1.5% and Ge is at most 0.1%; about 0.3% to 1.3% of Cu wherein Cu is less than (Si+Sn+Ge); V and Ti, wherein (V+Ti) is about 0.15 to 1.25%; at most 0.25% of Al; and a balance of Fe and incidental impurities, the sum of said alloying elements of said steel, except for Cr, being less than 9.0% of the weight, whereby
- Claim 2Independent Claim
The
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗