Medium temperature coating material for high speed turbomachinery and method of coating same

8Forward Citations (#13176776 Global)
0.5/yrCitation Velocity (#14937294 Global)
1.97Citation PageRank (#14849269 Global)
13Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the present invention may provide a coating material having heat resistance, abrasion resistance and low friction characteristics, which is coated on an operating component such as a rotating shaft working at a high speed without oil supply in a medium temperature environment (400° C.˜500° C.). This is so that the operating body can sufficiently withstand friction, heat generation and abrasion caused by contact with a bearing. The coating material of the present invention comprises 15 to 25 wt % antimony trioxide (Sb 2 O 3 ), 50 to 70 wt % binder, 10 to 20 wt % tungsten disulphide (WS 2 ) and 5 to 15 wt % silver (Ag). The binder comprises 60 to 80 wt % nickel (Ni) and 20 to 40 wt % chromium (Cr).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 8.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A coating material for a surface of an operating component of a machinery, comprising: 15 to 25 wt % antimony trioxide (Sb 2 O 3 ); 50 to 70 wt % binder; 10 to 20 wt % tungsten disulphide (WS 2 ); and 5 to 15 wt % silver (Ag), wherein the binder comprises 60 to 80 wt % nickel (Ni) and 20 to 40 wt % chromium (Cr).

  2. Claim 2Independent Claim

    A coating material for a surface of an operating component of a machinery, comprising: 15 to 25 wt % antimony trioxide (Sb 2 O 3 ); 40 to 65 wt % binder; 10 to 20 wt % tungsten disulphide (WS 2 ); 5 to 15 wt % silver (Ag); and 5 to 15 wt % molybdenum oxide (MoO 3 ), wherein the binder comprises 60 to 80 wt % nickel (Ni) and 20 to 40 wt % chromium (Cr).

  3. Claim 3Depends on #1

    The coating material of claim 1 , wherein the binder further comprises greater than 0 to 10 wt % aluminum (Al) based on a gross weight of the nickel and the chromium.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗