Patents
US 8,070,843 B2#51720773 Most CitedActiveUnited States (USPTO)Utility

Polishing fluids and methods for CMP

1Forward Citations (#51720773 Global)
0.1/yrCitation Velocity (#50835587 Global)
0.84Citation PageRank (#51720773 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Provided are several polishing compositions useful for modifying a surface, such as a semiconductor wafer suitable for fabrication of a semiconductor device, especially when used in fixed abrasive planarization techniques. The polishing compositions include a synergistic mixture of water, an oxidizing agent, a complexing agent, and metal ions. Also provided are various methods of surface planarization.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A chemical mechanical polishing system comprising: a fixed abrasive pad; and a polishing composition useful for modifying a surface of a wafer, the composition comprising a synergistic homogeneous mixture of water; an oxidizing agent; a complexing agent; and metal ions; wherein a majority of the complexing agent is selected from a simple monofunctional acid, a simple difunctional acid, a salt thereof, or a combination thereof, further wherein the mole ratio of complexing agent to metal ions present in the liquid is at least 3 to 1, and additionally wherein the mixture is substantially free of

  2. Claim 2Depends on #1

    The polishing system of claim 1 , wherein the fixed abrasive pad comprises a plurality of three-dimensional abrasive composites fixed to an abrasive article, wherein the abrasive composites comprise a plurality of abrasive particles fixedly dispers

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,341,384 ADissolution of metal with acidified hydrogen peroxide containing dibasic acid196729
US 3,754,878 AAbrasive cleaning compositions197317
US 3,756,957 ASolutions for chemical dissolution treatment of metallic materials197340
US 3,877,938 AEtch-bleaching method197526
US 4,130,454 AEtchant and process of etching with the same197838
US 4,954,142 AMethod of chemical-mechanical polishing an electronic component substrate and polishing slurry therefor1990329
US 4,987,099 AMethod for selectively filling contacts or vias or various depths with CVD tungsten199191
US 5,014,468 APatterned coated abrasive for fine surface finishing1991257
US 5,084,071 AMethod of chemical-mechanical polishing an electronic component substrate and polishing slurry therefor1992252
US 5,354,490 ASlurries for chemical mechanically polishing copper containing metal layers1994232
US 5,453,312 AAbrasive article, a process for its manufacture, and a method of using it to reduce a workpiece surface1995100
US 5,454,844 AAbrasive article, a process of making same, and a method of using same to finish a workpiece surface1995155
US 5,527,423 AChemical mechanical polishing slurry for metal layers1996529
US 5,692,950 AAbrasive construction for semiconductor wafer modification1997244
US 5,700,383 ASlurries and methods for chemical mechanical polish of aluminum and titanium aluminide1997172
WO 9,823,408 A1A composition and slurry useful for metal cmp—17
EP 0,846,742 A2Chemical mechanical polishing slurry useful for copper substrates—121
US 5,770,095 APolishing agent and polishing method using the same1998401
US 5,820,450 AAbrasive article having precise lateral spacing between abrasive composite members199870
WO 9,849,723 A1Method of planarizing the upper surface of a semiconductor wafer—162
US 5,897,375 AChemical mechanical polishing (CMP) slurry for copper and method of use in integrated circuit manufacture1999320
US 5,897,426 AChemical mechanical polishing with multiple polishing pads1999157
US 5,958,288 AComposition and slurry useful for metal CMP1999204
US 5,958,794 AMethod of modifying an exposed surface of a semiconductor wafer1999540
US 5,980,775 AComposition and slurry useful for metal CMP1999134
CN 1,242,729 AComposition and slurry useful for metal CMP—36
CN 1,254,441 AMethod of planarizing upper surface of semiconductor wafer—22
US 6,068,787 AComposition and slurry useful for metal CMP2000156
US 6,177,026 B1CMP slurry containing a solid catalyst200193

Non-Patent Literature (5)

  • Farkas et al., "Oxidation and Etching of Tungsten in CMP Slurries", pp. 25-32, Materials Research Society 1995.
  • Guthrie et al., "Chemical-Mechanical Polishing to Planarize Blanket and Selective CVD Tungsten", pp. 527-533, Materials Research Society 1992.
  • Kaufman et al., "Chemical-Mechanical Polishing for Fabricating Patterned W Metal Features as Chip Interconnects", J. Electrochem. Soc., vol. 138, No. 11, pp. 3460-3465, Nov. 1991.
  • Kim et al., "Self-Conditioning Fixed Abrasive Pad in CMP", Journal of the Electrochemical Society, 151 (12), pp. G858-G862 (2004).
  • Leidheiser, Jr., "The Corrosion of Copper, Tin, and Their Alloys", John Wiley and Sons, Inc., The Electrochemical Society, Inc., New York, NY, pp, 119-123 (1971).