Semiconductor storage device including a gate insulating film with a favorable nitrogen concentration profile and method for manufacturing the same
Abstract
A semiconductor storage device with excellent electrical characteristics (write/erase characteristics) by favorable nitrogen concentration profile of a gate insulating film, and a method for manufacturing the semiconductor device. The semiconductor device fabricating method operates by transferring charges through a gate insulating film formed between a semiconductor substrate and a gate electrode, including introducing an oxynitriding species previously diluted by plasma excitation gas into a plasma processing apparatus, generating an oxynitriding species by a plasma, and forming an oxynitride film on the semiconductor substrate as the gate insulating film. The oxynitriding species contains NO gas at a ratio of 0.00001 to 0.01% to the total volume of gas introduced into the plasma processing apparatus.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for fabricating a semiconductor storage device that operates by transferring a charge through a gate insulating film formed between a semiconductor substrate and a gate electrode, comprising: forming an oxide film on said semiconductor substrate; introducing an oxynitriding species previously diluted by plasma excitation gas, into a plasma processing apparatus; generating the oxynitriding species by a plasma; forming an oxynitride film on said semiconductor substrate as said gate insulating film by performing plasma oxynitridation with the oxynitriding species on the oxide film, the p
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 8,324,699 B2 | Method for manufacturing semiconductor device | 2012 | 42 |
| US 2011089425 A1 | Method for manufacturing semiconductor device | — | 4 |
References Cited — Backward Prior Art (15)
Non-Patent Literature (5)
- David C. T. Or, et al., "Enhanced reliability for low-temperature gate dielectric of MOS devices by N2O or NO Plasma nitridation", Microelectronics Reliability, 43, 2003, pp. 163-166.
- David C. T., et al., "Enhanced Reliability for Gate Dielectric of Low-Temperature Polysilicon Thin-Film Transistors by No-Plasma Nitridation", Proceedings, 2002 IEEE Hong Kong Electron Devices Meeting, pp. 35-38, 2002.
- H.G. Pomp et al., "lightly N2O nitrided dielectrics . . . ", Tech. Dig. IEDM, 1993, p. 463.
- Jonghan Kim, et al., "Scaling Down of Tunnel Oxynitride in Nand Flash Memory: Oxynitride Selection and Reliabilities", Reliability Physics Symposium, 35TH Annual Proceedings, IEEE International, pp. 12-16, 1997.
- Office Action issued Sep. 29, 2010 in EP Application No. 05 787 588.2.