Patents
US 8,066,916 B2#44535397 Most CitedActiveUnited States (USPTO)Utility

Synthesis of crystalline nanometric LiFeMPO4

2Forward Citations (#44535397 Global)
0.1/yrCitation Velocity (#41892031 Global)
0.90Citation PageRank (#47591479 Global)
25Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to lithium secondary batteries and more specifically to positive electrode materials operating at potentials greater than 2.8 V vs. Li + /Li in non-aqueous electrochemical cells. In particular, the invention relates to crystalline nanometric olivine-type LiFe 1-x M x PO 4 powder with M is Co and/or Mn, and 0<x<1, with small particle size and narrow particle size distribution. A direct precipitation process is described, comprising the steps of:—providing a water-based mixture having at a pH between 6 and 10, containing a dipolar aprotic additive, and Li (I) , Fe (II) , P (V) , and Co (II) and/or Mn (II) as precursor components;—heating said water-based mixture to a temperature less than or equal to its boiling point at atmospheric pressure, thereby precipitating crystalline LiFe 1-x M x PO 4 powder. An extremely fine particle size is obtained of about 80 nm for Mn and 275 nm for Co, both with a narrow distribution. The fine particle size is believed to accounts for excellent high-drain properties, while minimizing the need for conductive additives. The narrow distribution facilitates the electrode manufacturing process and ensures a homogeneous c

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A crystalline LiFe 1-x Co x PO 4 powder with 0<x<1, for use as electrode material in a battery, having a particle size distribution between 50-100 nm, with a ratio (d90-d10)/d50 of less than 1.5, wherein the powder does not include a conductive carbon coating.

  2. Claim 2Depends on #1

    The LiFe 1-x Co x PO 4 powder of claim 1 , wherein the maximum particle size is less than or equal to 100 nm.

  3. Claim 3Depends on #1

    The LiFe 1-x Co x PO 4 powder of claim 1 , wherein the particle size distribution is mono-modal.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (25)

PatentTitleYearCitations
US 5,910,382 ACathode materials for secondary (rechargeable) lithium batteries19992,380
WO 02,083,555 A2Binary, ternary and quaternary lithium phosphates, method for the production thereof and use of the same—66
WO 02,099,913 A1Lithium transition-metal phosphate powder for rechargeable batteries—58
US 2003215718 A1Fibrous articles and electrode systems—9
WO 2004/001881 A2Carbon-coated li-containing powders and process for production thereof—44
JP 2004079276 APositive electrode activator and its manufacturing method—74
US 6,749,967 B2Positive electrode active material and non-aqueous electrolyte cell200470
WO 2004/056702 A2Method for preparing insertion compounds of an alkali metal, active materials containing same, and device comprising said active materials—6
US 2004175614 A1Lithium transition-metal phosphate powder for rechargeable batteries—54
JP 2004259470 APositive electrode active material for lithium ion battery, and lithium ion battery having it—24
WO 2005/051840 A1Lithium metal phosphates, method for producing the same and use thereof as electrode material—78
US 2006035150 A1Carbon-coated li-containing powders and process for production thereof—53
US 2006035148 A1Novel electrodes for li-based electrochemical energy storage devices and a li-based electrochemical storage device—35
KR 20060025842 APreparation method of lithium iron phosphate—4
WO 2006/105848 A2Crystalline ion-conducting nanomaterial and method for the production thereof—17
WO 2007/000251 A1Crystalline nanometric lifepo4—29
US 2007031732 A1Nanoscale ion storage materials—88
WO 2008/018633 A1Compound having olivine structure, method for producing the same, positive electrode active material using compound having olivine structure, and nonaqueous electrolyte battery—33
US 7,390,472 B1Method of making nanostructured lithium iron phosphate—based powders with an olivine type structure200844
WO 2008/077447 A1SYNTHESIS OF ELECTROACTIVE CRYSTALLINE NANOMETRIC LiMnPO4 POWDER—35
WO 2008/077448 A1SYNTHESIS OF CRYSTALLINE NANOMETRIC LiFeMPO4—21
WO 2008/113570 A1Room temperature single phase li insertion/extraction material for use in li-based battery—11
US 2008241690 A1Crystalline Nanometric LiFePO4—38
US 2010086852 A1Room Temperature Single Phase Li Insertion/Extraction Material for Use in Li-Based Battery—18
US 7,771,628 B2Electrodes comprising mixed active particles201021

Non-Patent Literature (5)

  • Amine et al., "Olivine LiCoPO4 as 4.8 V Electrode Material for Lithium Batteries," Electrochemical and Solid-State Letters, vol. 3, No. 4, (2000), pp. 178-179.
  • Arnold et al., "Fine-Particle Lithium Iron Phosphate LiFePO4 Synthesized by a New Low-Cost Aqueous Precipitation Technique," Journal of Power Sources, vol. 119-121, (2003), pp. 247-261, Search Report.
  • Arumugan et al "Synthesis and electrochemical characterizations of nano-crystalline LiFePO4 . . . ", J. Solid Sate Electrochem (2009) 13:301-307.
  • Chen et al., "Reducing Carbon in LiFePO4/C Composite Electrodes to Maximize Specific Energy, Volumetric Energy, and Tap Density," Journal of the Electrochemical Society, vol. 149, No. 9, (2002), pp. A1184-A1189.
  • Delacourt et al., "Low Temperature Preparation of Optimized Phosphates for Li-Battery Applications," Solid State Ionics, vol. 173, (2004), pp. 113-118, Search Report.