Super-solution homogeneous propylene polymerization
Abstract
Processes for polymerizing propylene. About 40 wt % to about 80 wt % propylene monomer, based on total weight of propylene monomer and diluent, and about 20 wt % to about 60 wt % diluent, based on total weight of propylene monomer and diluent, can be fed into a reactor. The propylene monomer can be polymerized in the presence of a metallocene catalyst and an activator within the reactor at a temperature of about 80° C. or more and a pressure of about 13 MPa or more to produce a polymer product in a homogenous system. About 20 wt % to about 76 wt % (preferably About 28 wt % to about 76 wt %) propylene monomer, based on total weight of the propylene monomer, diluent, and polymer product, can be present at the reactor exit at steady state conditions.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A continuous process for polymerizing propylene, comprising: (a) feeding about 40 wt % to about 80 wt % propylene monomer, based on total weight of propylene monomer and diluent, and about 20 wt % to about 60 wt % diluent, based on total weight of propylene monomer and diluent, into a reactor; (b) polymerizing the propylene monomer in the presence of a metallocene catalyst and an activator within the reactor at a temperature of about 80° C. or more and a pressure of about 13 MPa or more to produce a polymer product in a homogenous system, wherein about 20 wt % to about 76 wt % propylene monome
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗