Manufacturing method of semiconductor device
Abstract
To provide a semiconductor device with high performance and low cost and a manufacturing method thereof. A first region including a separated (cleavage) single-crystal semiconductor layer and a second region including a non-single-crystal semiconductor layer are provided over a substrate. It is preferable that laser beam irradiation be performed to the separated (cleavage) single-crystal semiconductor layer in an inert atmosphere, and laser beam irradiation be performed to the non-single-crystal semiconductor layer in an air atmosphere at least once.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A manufacturing method of a semiconductor device comprising: forming a non-single-crystal semiconductor film over a substrate; removing a part of the non-single-crystal semiconductor film, which is in a first region over the substrate, to form a non-single-crystal semiconductor layer in a second region over the substrate; introducing ion species into a single-crystal semiconductor substrate to form an ion layer at a predetermined depth from a surface of the single-crystal semiconductor substrate; forming a bonding layer over the surface of the single-crystal semiconductor substrate; bonding th
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (22)
Non-Patent Literature (2)
- Zehner et al., "Preparation of atomically clean silicon surfaces by pulsed laser irradiation", Applied Physics Letters vol. 36, No. 1 (1980): pp. 56-59.
- Zehner et al., "Preparation of atomically clean silicon surfaces by pulsed laser irradiation," Applied Physics Letters, vol. 36, No. 1, Jan. 1, 1980, pp. 56-59.