Readily degradable resin composition and biodegradable container using the same
Abstract
Disclosed is a readily degradable resin composition having excellent biodegradability. Specifically disclosed is a readily degradable resin composition comprising: an aliphatic polyester (A) which has biodegradability; and an aliphatic polyester (B) which has a solution viscosity (η inh) of 0.25 dl/g or less as measured in a mixed solvent composed of m-chlorophenol and 1,2,4-trichlorobenzene at a weight-based ratio of 4:1 at a concentration of 0.4 g/dl and at a temperature of 30° C. and a melt viscosity of 50 Pa S or less as measured at 190° C. at a shear rate of 1 rad/s and is capable of biodegraded at a more rapid degradation rate than the aliphatic polyester (A). Also disclosed is a readily degradable resin composition comprising: an aliphatic polyester (A) which has biodegradability; and an aliphatic polyester (B′) which, when hydrolyzed, can release an acid showing a pH value of 2.0 or less when dissolved in water at a concentration of 0.005 g/ml and is capable of biodegraded at a more rapid degradation rate than the aliphatic polyester (A). Further disclosed is a biodegradable container comprising the readily degradable resin composition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A readily degradable resin composition comprising: an aliphatic polyester (A) which is biodegradable; and an aliphatic polyester (B) dispersed in said aliphatic polyester (A), which is biodegradable at a higher degradation rate than that of the aliphatic polyester (A) and which has a melt viscosity of 50 Pa·S or less at 190° C. and at a shear rate of 1 rad/s or a solution viscosity (η inh) of 0.25 dl/g or less measured under conditions of a concentration of 0.4 g/dl and of a temperature of 30° C. in a solvent of m-chlorophenol and 1,2,4-trichlorobenzene mixed at a weight ratio of 4:1, wherein
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (4)
- Database WPI, Week 200657, Thomson Scientific, London, GB; AN 2006-559944 & WO 2006/083044 A1; Aug. 10, 2006; XP-002608590.
- Official Action issued on May 20, 2011 for Chinese Patent Application No. 200780043797.1.
- Search Report and Written Opinion for PCT/JP2007/068633 dated Jul. 17, 2007.
- Supplementary European Search Report for EP 07 82 8406, Nov. 23, 2010.