Patents
US 8,047,039 B2#23286109 Most CitedActiveUnited States (USPTO)Utility

Process for producing stainless steel pipe

4Forward Citations (#23286109 Global)
0.3/yrCitation Velocity (#27388383 Global)
1.75Citation PageRank (#17987500 Global)
10Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for stainless-steel pipe production which comprises piercing rolling a raw material stainless steel containing, by mass, Cr: 10-30%, to give a hollow shell, elongating rolling the hollow shell using a mandrel bar, together with a graphite-free lubricant, to give a finishing rolling blank pipe and heating the blank pipe in a reheating furnace and subjecting the same to finishing rolling by sizing rolling to produce a hot-finished pipe, and then subjecting this pipe as a mother pipe to cold working to produce a stainless-steel pipe. In the reheating furnace, the finishing rolling blank pipe is heated to 1000° C. or more and subjected to heating in which an oxidizing gas is blown into the pipe inside, whereby a stainless-steel pipe which is inhibited from forming a carburized layer in the pipe inner surface can be produced. When the finishing rolling by sizing rolling to give a cold working mother pipe is carried out by stretch reducer rolling at 860-1050° C., an annealing heat treatment of the mother pipe for cold working can be omitted. Thus, a stainless-steel pipe having excellent surface quality can be efficiently produced.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 4.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing stainless steel pipes by subjecting a stainless steel raw material containing, by mass, Cr: 10-30%, to piercing rolling to give a hollow shell, subjecting the hollow shell to elongating rolling to give a finishing rolling blank pipe using a mandrel bar, together with a graphite-free lubricant, and heating the blank pipe in a reheating furnace and subjecting the heated blank pipe to finishing rolling by sizing rolling, wherein the finishing rolling blank pipe is subjected to heating in which it is heated to a temperature not less than 1000° C. in the reheating furnace an

  2. Claim 2Independent Claim

    A process for producing stai

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • International Preliminary Report on Patentability from the International Bureau of WIPO, dated Nov. 17, 2008.
  • International Search Report in corresponding PCT/JP2007/068362 dated Jul. 17, 2007.
  • Written Opinion of the ISA in corresponding PCT/JP2007/068362 dated Jul. 17, 2007 in Japanese language only.