Abstract

The present invention provides a porous semiconductive structure, characterized in that the structure has an electrical conductivity of 5·10 −8 S·cm −1 to 10 S·cm −1 , and an activation energy of the electrical conductivity of 0.1 to 700 meV, and a solid fraction of 30 to 60% by volume, and a pore size of 1 nm to 500 nm, the solid fraction having at least partly crystalline doped constituents which are bonded to one another via sinter necks and have sizes of 5 nm to 500 nm and a spherical and/or ellipsoidal shape, which comprise the elements silicon, germanium or an alloy of these elements, and also a process for producing a porous semiconductive structure, characterized in that A. doped semimetal particles are obtained, and then B. a dispersion is obtained from the semimetal particles obtained after step A, and then C. a substrate is coated with the dispersion obtained after step B, and then D. the layer obtained after step C is treated by means of a solution of hydrogen fluoride in water, and then E. the layer obtained after step D is treated thermally to obtain a porous semiconductive structure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for producing a porous semiconductive structure, wherein A. doped semimetal particles are obtained, and then B. a dispersion is obtained from the semimetal particles obtained after step A, and then C. a substrate is coated with the dispersion obtained after step B, and then D. the layer obtained after step C is treated by means of a solution of hydrogen fluoride in water, and then E. the layer obtained after step D is treated thermally to obtain a porous semiconductive structure.

  2. Claim 2Depends on #1

    A process according to claim 1 , wherein, in step A, continuously, (a) at least one vaporous or gaseous semimetal hydride selected from silane, germanium hydride and a mixture of these semimetal hydrides and at least one vaporous or gaseous dopant, and an inert gas are transferred into a reactor and mixed there, the proportion of the semimetal hydride being from 0

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗