Patents
US 8,043,692 B2#15977844 Most CitedExpiredUnited States (USPTO)Utility

Alloyed tungsten produced by chemical vapour deposition

7Forward Citations (#15977844 Global)
0.5/yrCitation Velocity (#17649373 Global)
1.43Citation PageRank (#24535929 Global)
39Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A wear-, erosion- and chemically-resistant material containing tungsten alloyed with carbon, the carbon being present in an amount of 0.01 wt % up to 0.97 wt % of the total weight, wherein the material preferably comprises a matrix of metallic tungsten with dispersed tungsten carbide nanoparticles having a particle size not greater than 50 nanometers, preferably not greater than 10 nanometers. The material is optionally also alloyed with fluorine, the fluorine being present in an amount of 0.01 wt % up to 0.4 wt % of the total weight. The material is extremely hard and tough.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 39 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A wear-resistant, erosion-resistant and chemically-resistant material comprising: metallic tungsten alloyed with carbon, the carbon being present in an amount of 0.01 wt % up to 0.97 wt % of the total weight, wherein the metallic tungsten is interdispersed with tungsten carbide nanoparticles having a particle size not greater than 50 nanometers, and wherein the tungsten carbide nanoparticles comprise tungsten monocarbide WC, tungsten semicarbide W 2 C, or a mixture of tungsten monocarbide WC and tungsten semicarbide W 2 C.

  2. Claim 2Depends on #1

    A material as claimed in claim 1 , additionally alloyed with fluorine, the fluorine being present in an amount of 0.001 wt % up to 0.4 wt % of the total weight.

  3. Claim 3Depends on #1

    A material as claimed in claim 1 , having a micro-hardness from 700 Hv up to 2000 Hv.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (39)

Non-Patent Literature (5)

  • International Preliminary Report Application No. PCT/GB2005/003913 Apr. 20, 2006.
  • International Search Report Application No. PCT/GB2005/003913 Dated Apr. 20, 2006.
  • J.V. Festa & J.C Danko "Some Effects of Fluorine Content on the Properties of Chemically Vapor Deposited Tungsten" General Electric Company, Nuclear Thermionic Power Operation, 1967, p. 349-361.
  • Khusainov M.A; "Thermal Strength of Refractory Materials Produced by Chemical Vapour Deposition of Gaseous" Leningrad, Leningrad State University Publishing House, 1979, p. 160.
  • Lakhokin Y.V., Krasovsky A.I;"Tungsten-Rhenium Coatings", (in Russian), Moscow, Nauka, 1989, p. 159.