Method for the production of fiber-reinforced polypropylene molded parts containing pores
Abstract
Low density and acoustically absorbing panels are produced by consolidation in a mold of a heated part of a pre-cut, lofty, semi-finished product containing polypropylene fibers and reinforcing fibers and having an air pore content of 20 to 80 vol.-% wherein overlapping with the periphery of the pre-cut part are heated strips of polypropylene optionally containing up to 60 wt.-% reinforcing fibers, but containing 5 vol.-% or less of air pores.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for the production of molded parts made of fiber-reinforced poly-propylene, wherein a pre-cut part A with a length of 1000 to 2000 mm and a width of 300 to 1000 mm of a flat semi-finished product made of fiber-reinforced polypropylene with a content of reinforcing fibers of 35 to 80 wt.-% and a content of uniformly distributed air pores of 20 to 80 vol.-% is heated to a temperature above the softening point of the polypropylene, placed into a two-part mold, pressed and thereby molded, wherein prior to molding one or several strips B with a width of 20 to 100 mm made of polypropylene w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗