US 8,043,444 B2#22250037 Most CitedActiveUnited States (USPTO)Utility

Steel wire for cold-formed spring excellent in corrosion resistance and method for producing the same

5Forward Citations (#22250037 Global)
0.3/yrCitation Velocity (#23219915 Global)
1.21Citation PageRank (#31709351 Global)
13Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A steel wire for a cold-formed spring according to the present invention contains a prescribed chemical component composition, wherein: a martensitic transformation start temperature M S1 shown by the following expression (1) is in the range from 280° C. to 380° C.; the austenite grain size number N of austenite grains is No. 12 or more; the grain boundary share of carbide precipitated along the austenite grain boundaries is 50% or less; the amount of retained austenite after austenitized and tempered is 20 vol. % or less; and the tensile strength is 2,000 MPa or more; M S1 =550−361[C]−39[Mn]−20[Cr] (1), where [C], [Mn] and [Cr] represent the contents (mass %) of C, Mn and Cr, respectively. Such a steel wire can: secure hot-rolling formability and subsequent drawability while aiming at higher strength and higher stress; moreover exhibit excellent corrosion resistance; and obtain a spring (mainly a suspension spring for an automobile) excellent also in fatigue strength which is a basic required characteristic.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A steel wire for a spring containing C: 0.45-0.54% (mass %, the same is applied hereunder), Si: 1.8-2.5%, Mn: 0.05-0.9% and Cr: 0.05-2.0%, comprising a fraction of martensite and bainite of 60% or less in area percentage, wherein P and S are controlled to 0.020% or less (including 0%), respectively; a martensitic transformation start temperature M S1 , shown by the following expression (1), is in the range from 280° C. to 380° C., where M S1 =550−361[C]−39[Mn]−20[Cr]  (1), and [C], [Mn] and [Cr] represent the contents (mass %) of C, Mn and Cr, respectively; and the steel wire has been austeniz

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Computer-generated English translation of Japanese patent 2004-143482, Hagiwara Hiroshi, May 20, 2004.
  • U.S. Appl. No. 11/348,409, filed Feb. 7, 2006, Kochi, et al.
  • U.S. Appl. No. 11/548,080, filed Oct. 10, 2006, Yoshihara, et al.
  • U.S. Appl. No. 11/559,654, filed Nov. 14, 2006, Yoshihara.
  • U.S. Appl. No. 11/583,703, filed Oct. 4, 2006, Yoshihara.