US 8,039,398 B2#45162750 Most CitedActiveUnited States (USPTO)Utility

Method of reducing non-uniformities during chemical mechanical polishing of excess metal in a metallization level of microstructure devices

2Forward Citations (#45162750 Global)
0.1/yrCitation Velocity (#41961025 Global)
0.87Citation PageRank (#49391042 Global)
36Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Prior to performing a CMP process for planarizing a metallization level of an advanced semiconductor device, an appropriate cap layer may be formed in order to delay the exposure of metal areas of reduced height level to the highly chemically reactive slurry material. Consequently, metal of increased height level may be polished with a high removal rate due to the mechanical and the chemical action of the slurry material, while the chemical interaction with the slurry material may be substantially avoided in areas of reduced height level. Therefore, a high process uniformity may be achieved even for pronounced initial surface topographies and slurry materials having a component of high chemical reactivity.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method, comprising: forming a metal layer comprising excess material that is positioned above an upper surface of a patterned dielectric layer formed above a substrate, said patterned dielectric layer comprising a first region and a second region; forming a cap layer on said metal layer; and completely removing said cap layer and removing a first portion of said excess material of said metal layer by chemical mechanical polishing, wherein a second portion of said excess material remains above an upper surface of said second region of said patterned dielectric layer after completely removing

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said cap layer has a higher chemical resistivity against a slurry used in said chemical mechanical polishing relative to said metal layer.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein forming said cap layer

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (36)

PatentTitleYearCitations
US 5,395,801 AChemical-mechanical polishing processes of planarizing insulating layers1995121
US 5,721,172 ASelf-aligned polish stop layer hard masking method for forming planarized aperture fill layers199898
US 5,827,782 AMultiple etch method for optimizing Inter-Metal Dielectric (IMD) spacer layer profile199820
US 5,840,629 ACopper chemical mechanical polishing slurry utilizing a chromate oxidant1998199
US 5,847,461 AIntegrated circuit structure having contact openings and vias filled by self-extrusion of overlying metal layer199820
US 5,920,792 AHigh density plasma enhanced chemical vapor deposition process in combination with chemical mechanical polishing process for preparation and planarization of intemetal dielectric layers199955
US 6,004,873 AMethod for reducing the pattern sensitivity of ozone assisted chemical vapor deposited (CVD) silicon oxide insulator layers199918
US 6,051,496 AUse of stop layer for chemical mechanical polishing of CU damascene2000143
US 6,096,652 AMethod of chemical mechanical planarization using copper coordinating ligands200047
US 6,114,234 AMethod of making a semiconductor with copper passivating film200010
US 6,114,246 AMethod of using a polish stop film to control dishing during copper chemical mechanical polishing200015
US 6,169,028 B1Method fabricating metal interconnected structure200126
WO 0,121,724 A1Slurry solution for polishing copper or tungsten—8
US 6,242,805 B1Method of using a polish stop film to control dishing during copper chemical mechanical polishing200114
US 6,258,711 B1Sacrificial deposit to improve damascene pattern planarization in semiconductor wafers200127
US 6,287,970 B1Method of making a semiconductor with copper passivating film200112
US 6,291,367 B1Method for depositing a selected thickness of an interlevel dielectric material to achieve optimum global planarity on a semiconductor wafer200119
US 6,300,653 B1Method for forming a high areal capacitance planar capacitor200122
US 6,391,707 B1Method of manufacturing a zero mask high density metal/insulator/metal capacitor200259
US 6,391,780 B1Method to prevent copper CMP dishing200231
US 2002096770 A1Viscous protective overlayers for planarization of integrated circuits—4
US 2002163029 A1Zero mask high density metal/insulator/metal capacitor—54
US 2002182886 A1Barrier film deposition over metal for reduction in metal dishing after CMP—5
US 2003054649 A1Method for reducing dishing in chemical mechanical polishing—6
US 2003203624 A1Manufacturing method of semiconductor device—33
US 6,646,323 B2Zero mask high density metal/insulator/metal capacitor200340
US 2004266188 A1Polishing method, metallization fabrication method, method for manufacturing semiconductor device and semiconductor device—11
US 2006003570 A1Method and apparatus for electroless capping with vapor drying—31

Non-Patent Literature (1)

  • Translation of Official Communication from German Patent Office for German Patent Application No. 10 2007 009 902.0-43 dated Oct. 16, 2007.