Patents
US 8,034,857 B2#18905824 Most CitedActiveUnited States (USPTO)Utility

Polyetherimide/polyphenylene ether sulfone blends

6Forward Citations (#18905824 Global)
0.4/yrCitation Velocity (#20052382 Global)
1.18Citation PageRank (#33107822 Global)
24Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Compositions comprise phase separated polyetherimide/polyphenylene ether sulfone blends. The dispersed phase has an average cross sectional size of 0.1 to 10 micrometers. The composition retains has good hydrolytic stability and is capable of withstanding steam autoclaving at temperatures of 130 to 138° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 6.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A composition comprising a phase separated blend comprising: 50 to 80 weight percent of a polyetherimide; and 20 to 50 weight percent of a polyphenylene ether sulfone; wherein the phase separated blend comprises a dispersed phase having an average cross-section of 0.01 to 10 micrometers; wherein the composition initially has a multiaxial impact energy of greater than or equal to 45 ft-lbs (61 Joules) and after 300 hours steam autoclave exposure at 130 to 138° C. has a multiaxial impact energy of greater than or equal to 20 ft-lbs (27 Joules), wherein multiaxial impact energy is determined acco

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 3,803,085 AMethod for making polyetherimides1974191
US 3,847,867 APolyetherimides1974379
US 3,852,242 AMethod for making polyetherimide1974240
US 3,905,942 AMethod for making polyetherimides and products produced thereby1975182
US 3,972,902 A4,4'-Isopropylidene-bis(3- and 4-phenyleneoxyphthalic anhydride)1976211
US 3,983,093 ANovel polyetherimides1976265
US 4,176,222 AProduction of aromatic polyethers1979168
US 4,293,670 ABlends of poly(aryl ether) resins and polyetherimide resins198173
US 4,443,591 AMethod for making polyetherimide1984184
US 4,455,410 APolyetherimide-polysulfide blends1984218
US 4,473,684 APoly (aryl ether)s198415
US 4,503,168 ACookware made from polyarylethersulfone198568
US 5,037,902 AMiscible blends of imide containing polymers with poly(aryl sulfones)199121
EP 0,440,433 A2Poly (arylene sulfide) - based thermoplastic polymer alloy—7
US 5,134,202 AProcess for miscible blends of imide containing polymers with poly(aryl sulfones)19929
US 5,191,305 AMultiple bandpass filter199360
US 5,212,259 AMiscible blends of imide containing polymers with poly(aryl sulfones)19938
US 5,286,812 AHigh performance blends of aromatic polyimides with aromatic polyethersulfones199412
US 5,917,137 AGas separation membranes of blends of polyethersulfones with aromatic polyimides199934
US 6,482,880 B1Poly(biphenyl ether sulfone) resins having improved UV yellowing resistance200224
US 2005113558 A1Polyethersulfone composition, method of making and articles therefrom—33
US 2006069236 A1Polyethersulfone compositions with high heat and good impact resistance—28
US 7,041,773 B2Polyimide sulfones, method and articles made therefrom200667
US 2006167216 A1Polyethersulfone composition, method of making and articles therefrom—19

Non-Patent Literature (5)

  • ASTM D1003, Standard Test Method for Haze and Luminous Transmittance of Transparent Plastics, 6 pages.
  • ASTM D1238, Standard Test Method for Melt Flow Rates of Thermoplastics by Extrusion Plastometer, 14 pages.
  • ASTM D3763, Standard Test Method for High Speed Puncture Properties of Plastics Using Load and Displacement Sensors, 9 pages.
  • ASTM D542, Standard Test Method for Index of Refraction of Transparent Organic Plastics, 4 pages.
  • ASTM D638, Standard Test Method for Tensile Properties of Plastics, 15 pages.