Abstract
It is an object to provide a method of manufacturing a crystalline silicon device and a semiconductor device in which formation of cracks in a substrate, a base protective film, and a crystalline silicon film can be suppressed. First, a layer including a semiconductor film is formed over a substrate, and is heated. A thermal expansion coefficient of the substrate is 6×10 −7 /° C. to 38×10 −7 /° C., preferably 6×10 −7 /° C. to 31.8×10 −7 /° C. Next, the layer including the semiconductor film is irradiated with a laser beam to crystallize the semiconductor film so as to form a crystalline semiconductor film. Total stress of the layer including the semiconductor film is −500 N/m to +50 N/m, preferably −150 N/m to 0 N/m after the heating step.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 6.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of manufacturing a semiconductor device comprising the steps of: forming a silicon nitride oxide film over a glass substrate having a thermal expansion coefficient ranging from 6×10 −7 /° C. to 38×10 −7 /° C.; forming a semiconductor film over the silicon nitride oxide film; heating the silicon nitride oxide film and the semiconductor film; and irradiating the heated semiconductor film with a laser beam, whereby a part of a surface of the glass substrate is softened, wherein the formation of the silicon nitride oxide film is carried out by using a source gas of a mixture of SiH 4 , N
- Claim 2Depends on #1
The method of manufacturing a semiconductor device according to claim 1 , wherein the laser beam is a continuous wave laser beam.
- Claim 3Independent Claim
The method of manufacturing a sem